Frit-Happens !

Tutorials in here.. => Books and etutorials => Topic started by: Dee Dee on October 01, 2012, 06:21:58 PM



Title: INNER DEPTH - A Glass Quilling Tutorial
Post by: Dee Dee on October 01, 2012, 06:21:58 PM

Eeek - I am ever so excited!  This is my first ever tutorial and I hope you like it!


(http://farm9.staticflickr.com/8462/8045048601_1b6c85ef2a.jpg) (http://www.flickr.com/photos/37221440@N06/8045048601/)
Inner Depth Tutorial Etsy first page (http://www.flickr.com/photos/37221440@N06/8045048601/) by Maid of Glass (http://www.flickr.com/people/37221440@N06/), on Flickr


In this e-book, I will show you how to make my signature style Inner Depth beads. Using step by step written instructions and photographs.  Plus a mini tutorial on how I achieve neatly encased bead holes when I am encasing my beads with little to no bleeding of the glass underneath.

Now available in my Etsy shop:

www.beadsbystephanie.etsy.com


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: JKC on October 02, 2012, 03:03:51 AM
The beads look lovely, I especially like the blue one.  Good luck with the tutorial.  Janet


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: chipperpottery on October 02, 2012, 03:08:27 AM
Finger slipped  ;)


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: Krysia@No98 on October 02, 2012, 03:08:55 AM
The front page looks great.  

I have noticed when I look at other peoples tutorials that they include a page or two from their tutorial, the equipment page and another page to give people an idea of the equipment they need and to show quality of the tutorial.


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: Dee Dee on October 02, 2012, 03:32:02 AM
The front page looks great. 

I have noticed when I look at other peoples tutorials that they include a page or two from their tutorial, the equipment page and another page to give people an idea of the equipment they need and to show quality of the tutorial.


Done!!  Thanks xx


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: Dee Dee on October 02, 2012, 03:33:19 AM
Finger slipped  ;)

Thanks Rita, it's been sent! ;D


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: chipperpottery on October 02, 2012, 04:11:34 AM
I have just had a peak, can't wait to have ago. But tomorrow is my torching day  :-\


Title: Re: INNER DEPTH - A Glass Quilling Tutorial
Post by: Krysia@No98 on October 02, 2012, 06:59:58 AM
The front page looks great. 

I have noticed when I look at other peoples tutorials that they include a page or two from their tutorial, the equipment page and another page to give people an idea of the equipment they need and to show quality of the tutorial.


Done!!  Thanks xx

Brill  ;D