Text only
|
Text with Images
Frit-Happens !
Tutorials in here.. => Lampworking => Tips and tricks => Topic started by: beadysam on January 11, 2007, 06:17:28 PM
Title:
Painted Beads 101
Post by:
beadysam
on
January 11, 2007, 06:17:28 PM
http://www.deborahread.com/painted_beads_101.htm
Title:
Re: Painted Beads 101
Post by:
LesleyMac
on
January 11, 2007, 06:23:39 PM
Sam this is fantastic and my paints are on the way from Bronwen Heilman so I can't wait to try it. ;D
Title:
Re: Painted Beads 101
Post by:
beadysam
on
January 11, 2007, 06:27:49 PM
Good-oh!
Text only
|
Text with Images