Text only
|
Text with Images
Frit-Happens !
Jewellery => Metal and wire => Topic started by: Les on March 31, 2011, 03:15:03 PM
Title:
wire gauge chart sticky
Post by:
Les
on
March 31, 2011, 03:15:03 PM
here you go ....
(http://i149.photobucket.com/albums/s76/mizgeorge/quickgauges.jpg)