Originally posted by Beck...
this is a site i came across a while ago got a tutorial for pot melts and some lovely pics too as well as a pattern bar tutorial that you might find fun to try as that might give to a closer result to moje !!
http://www.clearwaterglass.com/Tutorials/TutorialAperturePour.html
check out the gallery section which is gorgeous with examples of where pot melts etc have been used in finished pieces
e.g. (http://www.clearwaterglass.com/GlassArt/MeridianSeries/Keys_7.jpg)
Ooo this is a different one to what Ive seen...... some good pics of the process though!! Thanks for link.... off a read ;D