I am just making sure.
So after it has had its first fire up with nothing in it . And I want to make some beads the kiln.
do i put it on the programme for garage what ever number lifesaver lee has put it on , as i want to put in kiln as i make , then just leave the programme to run its course as i make the beads . Then leave the kiln doing its thing over night ??? Maxi kiln by the way so kaz if you are there !!! please please please
Hi Stacey.
Yes, just press the start button then 1 will run whilst you're working. Once you're finished if you press and hold the up arrow for about 6 seconds, the programme will move onto the next segment (2) and you can go to bed. Then in the morning your beads should be nearly cool enough to take out and admire ;D