Frit-Happens !

Tutorials in here.. => Beginner beadmaking basics & colour charts => Topic started by: Deesigned Beads on March 23, 2009, 08:13:25 AM



Title: Wavey ribbon tutorial
Post by: Deesigned Beads on March 23, 2009, 08:13:25 AM
Here is a link to another tutorial available on my blog:

http://deesignedbeads.blogspot.com/2008/11/one-of-those-days.html

Enjoy!
Diana


Title: Re: Wavey ribbon tutorial
Post by: Steampunkglass on March 23, 2009, 08:23:20 AM
Cheers! Excellent tutorial, really nice and clear pictures! ;D


Title: Re: Wavey ribbon tutorial
Post by: TiaraHelen on March 23, 2009, 08:25:50 AM
Thanks dee, I've been peeping at your tutorials while you've been putting them up - very helpful.


Title: Re: Wavey ribbon tutorial
Post by: Deesigned Beads on March 23, 2009, 08:38:29 AM
Glenn, you are welcome!  And Helen, peep away, lol. 

I would really love to see what other pple do with this tutorial!

Diana


Title: Re: Wavey ribbon tutorial
Post by: Vicki.White on April 17, 2009, 05:16:29 PM
Awesome I will be trying this one tomorrow!!! thanks !!


Title: Re: Wavey ribbon tutorial
Post by: Im a glassy babe on April 17, 2009, 05:39:49 PM
Great tutorial, thanks!  ;D