Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Findings, Fixtures & Display => Topic started by: Bluebottle on November 06, 2008, 10:26:08 AM

Title: DICHROIC BLANKS
Post by: Bluebottle on November 06, 2008, 10:26:08 AM
Can anyone tell me where in the UK I can get round dichroic fusing blanks about 35mm in diameter, I can find them in the US of A but postage is a bit prohibitive on a small quantity, any help greatly appreciated  ::)

Mike   ;D
Title: Re: DICHROIC BLANKS
Post by: mjbelkin on November 06, 2008, 10:41:32 AM
Have Warm Glass (http://www.warm-glass.co.uk/) got anything of use?
Title: Re: DICHROIC BLANKS
Post by: Zeldazog on November 07, 2008, 09:25:26 AM
You're right, they do, Mel, I thought I had seen them (just wasn't sure where!)

http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=456 (http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=456)
Title: Re: DICHROIC BLANKS
Post by: Bluebottle on November 07, 2008, 05:28:40 PM
Thanks guys but these aren't quite what I  want, what i'm looking for is the round dichroic pieces before they are fused   ::)

Mike   ;D
Title: Re: DICHROIC BLANKS
Post by: Zeldazog on November 07, 2008, 05:37:40 PM
Never seen those Mike to be honest (then again, I don't look for dichroic)
Title: Re: DICHROIC BLANKS
Post by: Soozintheshed on November 07, 2008, 06:03:10 PM
What you after Mike?  The stainless steel settings?

I have some on order if so, not sure of the pricing yet though.
Title: Re: DICHROIC BLANKS
Post by: Bluebottle on November 07, 2008, 07:55:29 PM
Quote from: Soozintheshed on November 07, 2008, 06:03:10 PM
What you after Mike?  The stainless steel settings?

I have some on order if so, not sure of the pricing yet though.

Nope it's the actual dichroic glass discs before they are fused that I'm looking for   ;)

Mike   ;D
Title: Re: DICHROIC BLANKS
Post by: sparrow on November 08, 2008, 12:08:17 PM
I guess like these, but round and in the UK - right?

http://cgi.ebay.com/60-Large-Dichroic-Diamonds-90-COE-Fusing-2-Sizes-90COE_W0QQitemZ390004294862QQcmdZViewItemQQimsxZ20081030?IMSfp=TL081030106009r36308
Title: Re: DICHROIC BLANKS
Post by: Zeldazog on November 08, 2008, 01:30:03 PM
These any good?

http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=974 (http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=974)

(there are other ones too)
Title: Re: DICHROIC BLANKS
Post by: greenbeadenvy on November 08, 2008, 02:53:51 PM
Quote from: Bluebottle on November 07, 2008, 05:28:40 PM
Thanks guys but these aren't quite what I  want, what i'm looking for is the round dichroic pieces before they are fused   ::)

Mike   ;D
Hi ya mike, Do want to make Dichroic glass pendants but are not too keen on using a glass cutter?  I have supprising news for you.... When I used to make Dichroic pendants in the old days they started out life... Square. Honest I'm not pulling your leg. Little square stacks go into the kiln and come out round.
Em xx
Title: Re: DICHROIC BLANKS
Post by: Bluebottle on November 08, 2008, 03:38:33 PM
Quote from: greenbeadenvy on November 08, 2008, 02:53:51 PM
Quote from: Bluebottle on November 07, 2008, 05:28:40 PM
Thanks guys but these aren't quite what I  want, what i'm looking for is the round dichroic pieces before they are fused   ::)

Mike   ;D
Hi ya mike, Do want to make Dichroic glass pendants but are not too keen on using a glass cutter?  I have supprising news for you.... When I used to make Dichroic pendants in the old days they started out life... Square. Honest I'm not pulling your leg. Little square stacks go into the kiln and come out round.
Em xx

Dawn : no sorry these aren't what I want   :)

Sabine : Yep but round and in this country ;)

Emma : Sounds an interesting technique   :o  any chance of parting with the info   ??? ::)

Mike  ;D








Title: Re: DICHROIC BLANKS
Post by: greenbeadenvy on November 08, 2008, 03:59:50 PM
Quote from: Bluebottle on November 08, 2008, 03:38:33 PM
Quote from: greenbeadenvy on November 08, 2008, 02:53:51 PM
Quote from: Bluebottle on November 07, 2008, 05:28:40 PM
Thanks guys but these aren't quite what I  want, what i'm looking for is the round dichroic pieces before they are fused   ::)

Mike   ;D
Hi ya mike, Do want to make Dichroic glass pendants but are not too keen on using a glass cutter?  I have supprising news for you.... When I used to make Dichroic pendants in the old days they started out life... Square. Honest I'm not pulling your leg. Little square stacks go into the kiln and come out round.
Em xx

Dawn : no sorry these aren't what I want   :)

Sabine : Yep but round and in this country ;)

Emma : Sounds an interesting technique   :o  any chance of parting with the info   ??? ::)

Mike  ;D


No problemo Mike, gimmee half hour to write something.
Em xx
Title: Re: DICHROIC BLANKS
Post by: greenbeadenvy on November 08, 2008, 04:25:15 PM
I'll be quick cuz my stew and dumplings is almost ready LOL.
Use Bullseye glass for the base cut about an inch square, add Dichroic glass cut to same size and then(this is the important bit) top the whole thing of with a piece of 3mm clear bullseye glass. Pop the little stacks in the kiln making sure they wont touch each other once they start melting. Then full fuse (around 800 degrees) The temperature may need adjusting slightly, it just depends on what kind of kiln you have.
The best advice I can give is make notes of every firing, like what temp you used, what you did wrong, what went right or what pattern of dichroic you used...anything that you think will be useful for the next firing.
Have a go, play around and have fun.
I bet if you have a looksie in 'youtube' or search the internet for a bit you will find lots of more detailed toots.
Em xx
Title: Re: DICHROIC BLANKS
Post by: Bluebottle on November 08, 2008, 04:35:54 PM
Quote from: greenbeadenvy on November 08, 2008, 04:25:15 PM
I'll be quick cuz my stew and dumplings is almost ready LOL.
Use Bullseye glass for the base cut about an inch square, add Dichroic glass cut to same size and then(this is the important bit) top the whole thing of with a piece of 3mm clear bullseye glass. Pop the little stacks in the kiln making sure they wont touch each other once they start melting. Then full fuse (around 800 degrees) The temperature may need adjusting slightly, it just depends on what kind of kiln you have.
The best advice I can give is make notes of every firing, like what temp you used, what you did wrong, what went right or what pattern of dichroic you used...anything that you think will be useful for the next firing.
Have a go, play around and have fun.
I bet if you have a looksie in 'youtube' or search the internet for a bit you will find lots of more detailed toots.
Em xx

Thanks Emma I'll give it a go   :D

Mike   ;D

Title: Re: DICHROIC BLANKS
Post by: Zeldazog on November 08, 2008, 04:38:12 PM
There's good information on Bullseye's own website, in their technotes section, that explains why this happens (I'll dig out the link)

Basically, glass likes to be around 6mm thick, so if you stack it thicker as Emma suggests, when it gets to the 800 degrees range, it will start to spread (it's footprint) outwards to make itself thinner. likewise, a small square, say only 8-10mm across, single thickness, will also go round - because it pulls into itself to get up to that thickness (not sure if this explains it or not!) - that said, a larger piece of only single thickness, taken to full fuse will start to pinch inwards but only along the sides, and not the corners.  



Title: Re: DICHROIC BLANKS
Post by: Zeldazog on November 08, 2008, 04:38:34 PM
Excellent mini-toot, Em!!
Title: Re: DICHROIC BLANKS
Post by: misspixie on November 08, 2008, 10:54:27 PM
Oooh... Might have to play at that next time I'm fusing! Thanks for the explanation Emma - and the science-y bit too Dawn!
Title: Re: DICHROIC BLANKS
Post by: Pat from Canvey on November 09, 2008, 09:23:08 AM
That's how broken beads make good cabochons after the bead release is cleaned away.
(http://pic20.picturetrail.com/VOL1426/5604171/20500169/342364455.jpg)
Just took this to show broken bead made into cabochon. Sorry the quality of the picture is poor, took it on the kitchen floor without using my tripod. It's about 1 inch in diameter.
Title: Re: DICHROIC BLANKS
Post by: nic on November 09, 2008, 09:26:26 AM
I also found that cutting the corners off the glass gave a better round.
Title: Re: DICHROIC BLANKS
Post by: Hotglass28 on November 11, 2008, 01:59:53 PM

I make these cabs for a living and there is no need to cut the corners.  As said before glass want to suck up and pull its edges in so rounds are the most easest shape to get.

you need at least two layers to get nice edges.  If you just have one layer then you normally get a haze around the edges where the glass has picked up the bat wash or fibre paper on the kiln shelf.

I fuse to 860 to achieve full rounds.

Happy fusing!