Frit-Happens !

Lampwork => Common Problems => Topic started by: Donna@Rockin' Beads on September 22, 2008, 07:29:24 PM

Title: Cleaning Cabochons
Post by: Donna@Rockin' Beads on September 22, 2008, 07:29:24 PM
OK, I have managed to make 4 cabochons (hopefully to be turned into 2 pairs of cufflinks, although the first 2 are decidedly dull and misshapen and the second pair are quite different in size from eachother ('well, they are handmade' I hear you all cry  ;D).
Anyway, so I've scrubbed the backs with a nail brush and just can't seem to get the last residue of bead release off them.
What do you guys do to clean them up?
Do I just have to keep soaking and scrubbing? (I seriously hate elbow grease!!!)
Title: Re: Cleaning Cabochons
Post by: Redhotsal on September 22, 2008, 07:32:32 PM
Wet'n'dry  :)
Title: Re: Cleaning Cabochons
Post by: Donna@Rockin' Beads on September 22, 2008, 07:33:26 PM
Ah, of course.
Thanks Sal  :-*