frit stringer and frit over a base colour (http://www.ozziebuddy.com/frittutes.html)
LE frit stringer thread (http://www.lampworketc.com/forums/showthread.php?t=27067)
You can also make easy twisties or latticino-cane with frit.
You need:
* any pale opaque color (for twisty) or clear (for latticino-cane)
* fritblend of choice
* a rod of clear.
How to make the cane:
1) Melt a big blob
2) roll blob in fritblend
3) melt in completely
4) encase in clear
5) reheat the blob, pull and twist.
That sounds fun, I am gonna try this next time I get near my torch ;D
Great tip Verena
THANK you :) Great advice!!!!
Wow - I'm going to try that too! Thanks :)