Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Tools and Presses => Topic started by: jojo on January 17, 2007, 11:09:25 AM

Title: Press?
Post by: jojo on January 17, 2007, 11:09:25 AM
Hiya

Could all you experienced guys tell me if there is such a thing as a button press.  I am looking for a sort of lentil type/button type shape?  I know what I mean ??? lol
Title: Re: Press?
Post by: Josephine on January 17, 2007, 12:03:33 PM
http://www.cattwalk.com/Buttons.htm
http://www.cattwalk.com/lentilsandcapsules.htm
hhttp://www.zooziis.com/index.asp?PageAction=VIEWCATS&Category=44
http://www.zooziis.com/index.asp?PageAction=VIEWCATS&Category=9

These should give you an idea of what is available.
Title: Re: Press?
Post by: Mary on January 18, 2007, 11:36:12 PM
I can recommend the Cattwalk button, it's the one I have. A nice press to use, and a nice range of sizes.
Title: Re: Press?
Post by: xtweeksx on January 19, 2007, 12:08:52 AM
I like the Cattwalk button, its a lovely shape.... I get all warm an fuzzy playing with them in my hands hehe

Jenx
Title: Re: Press?
Post by: ♥♥Tan♥♥ on January 19, 2007, 06:04:51 PM
have you decided yet Jo?
Title: Re: Press?
Post by: Trudi on March 23, 2007, 10:54:38 PM
Hi

I've looked at these - how do yo match up the top & bottom when pressing? And they easy enough for a newbie to have go on?

Thanks

T
Title: Re: Press?
Post by: CelticGlass on March 23, 2007, 11:06:26 PM
Quote from: shine-on2 on March 23, 2007, 10:54:38 PM
Hi

I've looked at these - how do yo match up the top & bottom when pressing? And they easy enough for a newbie to have go on?

Thanks

T

I make buttons in one of Martins doming blocks and they come out like half a lentil. Good enough to do several commision sets for bridalware in the past. Page boy outfit buttons too.

I'll do a tutorial if enough members wanna see it  ?







Title: Re: Press?
Post by: Dragonfire Glass on March 23, 2007, 11:08:12 PM
yes please to a tut
Title: Re: Press?
Post by: Vicki on March 23, 2007, 11:09:56 PM
yes please, I have a small lentle masher from Martins site, not used it yet & not sure if I'll get on with it....maybe I should have a go with it ;D
Title: Re: Press?
Post by: Mary on March 23, 2007, 11:18:31 PM
Trudi, Cattwalk presses are best with a guide base, they do an offer of a base and press for $80. Or get a Zooziis one, they have pins built in. Like anything, there are tricks to presses, but they are pretty easy to use. The Cattwalk site has tutorials for most of their presses.
Title: Re: Press?
Post by: CelticGlass on March 23, 2007, 11:25:41 PM
Quote from: Failariel on March 23, 2007, 11:08:12 PM
yes please to a tut

Okey Dokey-- will get camera going during tomorrows session.  More bead porn I guess.

Title: Re: Press?
Post by: Trudi on March 24, 2007, 08:33:10 AM
Hi

I was looking at the catwalk & Zooziis - and I could see that catwalk offer a base - but I can't see from the site how that would help you line up the top & bottom pieces!
Title: Re: Press?
Post by: Caroline on March 24, 2007, 08:47:33 AM
with cattwalk presses theres a pin that you line the bottom of the press to, tighten the screws and then when your pressing a bead you line the top up to the bottom by using the pin
Title: Re: Press?
Post by: LesleyMac on March 25, 2007, 08:34:07 AM
Don't be put off because you can't visualise how it works, its really easy honestly.

You put the bottom part of your press tool in the base and tighten it, (really easy) then when you are ready to press you do that with the top part, because the base has two "sides" you can locate easily, you just need to make sure that the two corners line up.  It really is easy.  The difficult part is getting the right amount of glass but that comes with experience and practice with the tool.


Good luck and hope you give it a try. ;D