I am feeling a bit negative towards my presses as I am finding it reallly, really difficult to get nice neat holes in them that are rounded rather than sharp. Making me feel a bit fed up as I can now get lovely puckers and nice even beads when making standard donuts.
This isn't lack of practice as I have made about 200!!!!! Some have turned out OK (mostly the deep lentil and the sleek pillow) but standard lentils, puffy pillows and some of the others, I am having no luck at all. I use Cattwalk but don't know if that makes any odds - as I am OK with using the locators.
Is it just me, or can anyone offer any hints and tips?
Thank You!
Kaz
Title: Re: Using presses - getting nice ends....
Post by: June on July 04, 2008, 08:48:59 PM
I'll be watching this thread with interest...!!  ;D
Title: Re: Using presses - getting nice ends....
Post by: Kaz on July 04, 2008, 08:50:28 PM
Are you struggling too then June? I am getting really fed up and have gone back to making round donuts for a while. Even resorted to making fritty donut sets today when I took a few hours off.
Kaz
Title: Re: Using presses - getting nice ends....
Post by: June on July 04, 2008, 08:52:09 PM
Yes, I am, Kaz, though I haven't practised too much, either.  I did make a lentil I was really pleased with earlier in the week, only for it to split in half when removing from the mandrel .. !  That's life !!
Title: Re: Using presses - getting nice ends....
Post by: turnedlight on July 04, 2008, 09:01:58 PM
With my pillow press, I make a fat barrel, but not quite as long as the press so that it squeezes towards the ends a bit, then I heat the ends pointing the flame along the mandrel at the hole, and as this makes the sides droop, I also use the marver to keep the ends flat. Having said all that, they're not always perfect, but it gets rid of sharp ends.
Hth, Kathryn x
Title: Re: Using presses - getting nice ends....
Post by: Mary on July 04, 2008, 09:48:12 PM
Build your bead on a footprint a mm or two shorter than the press, marver a bit before pressing like Kathryn says, and find the right pressing temp - don't press when the glass is too runny hot, or it will all squish out the ends. Let it form a skin first. Hope that helps!
Title: Re: Using presses - getting nice ends....
Post by: Kaz on July 04, 2008, 09:50:05 PM
Thanks both - it seems likely that as I like my torch very hot, I am probably putting them in too runny. ;D
Kaz
Title: Re: Using presses - getting nice ends....
Post by: Jolene on July 05, 2008, 07:15:01 AM
I found a nice tut recently where you make small beads first...lemme go find it again
Title: Re: Using presses - getting nice ends....
Post by: Jolene on July 05, 2008, 07:16:04 AM
http://www.frit-happens.co.uk/forum/index.php?topic=7331.0

X Jo
Title: Re: Using presses - getting nice ends....
Post by: firedinglass on July 05, 2008, 01:28:43 PM
I was looking on Lampwork etc. and Andre Guarini (spelling?) has just started selling a new tool specifically for making neat ends. It is basically a graphite marver with a narrow channel made in top to rest the mandrel in so that you can push right up to the end of the bead, I think it might also have been slightly bevelled.  Someone commented it would be easy to adapt any graphite marver to do this.  Sorry I'm not computer good enough to add link! Perhaps someone less of a technophobe can! hope this is of some use :)
Title: Re: Using presses - getting nice ends....
Post by: Shirley on July 05, 2008, 01:49:47 PM
Ah, now that might be the marver that Judith Johnston used at the flame off
Title: Re: Using presses - getting nice ends....
Post by: firedinglass on July 07, 2008, 06:35:08 PM
Arrow Springs sell the tool I'm talking about but it's pricey...
Title: Re: Using presses - getting nice ends....
Post by: Vicki on July 07, 2008, 06:45:51 PM
I've found some presses are mandrel specific aswell Kaz, try using a larger or smaller mandrel depending on what your using now.  I also do what mary says & make my footprint a wee bit smaller & I let the glass settle for a few seconds in the bottom of the press before I squish, it works for me anyway ;D
Title: Re: Using presses - getting nice ends....
Post by: Ilona on July 07, 2008, 08:12:12 PM
I always make my footprint a little bit smaller then when I have made about 3/4 of the size of the bead I marver it into a cube shape,this makes nice ends, then press and add more glass as required This works for me  :)
Title: Re: Using presses - getting nice ends....
Post by: SueP on July 07, 2008, 09:11:43 PM
I use the top of the press and marver the bead in that to get an olive shape slightly shorter than the required length then put another wrap round the middle :)  I think we all develop our own techniques  ;D ;D
Title: Re: Using presses - getting nice ends....
Post by: Kaz on July 07, 2008, 10:09:35 PM
Well it certainly sounds like it! ;D I am working my way through these hints and tips and starting to have more success!
Kaz
Title: Re: Using presses - getting nice ends....
Post by: saffie on July 07, 2008, 10:14:30 PM
i too am quite despondant about my ends!!! I tried a few of those hints but will try again methinks it is all PPP but so hard when all you wanna do is lob the press!!! (not advisable really!!!)
Title: Re: Using presses - getting nice ends....
Post by: Mary on July 07, 2008, 10:49:44 PM
Remember you don't need to just press once. When I'm doing big beads I press in stages. I rarely fill all the corners on a first press even if the glass amount is perfect. I gently press once, to get the rough shape, then reheat and press again and it will look better. I can repeat this several times to get a nice even bead, without needing to press while it's too runny.
Title: Re: Using presses - getting nice ends....
Post by: Trudi on July 19, 2008, 10:23:11 PM
Quote from: Mary on July 07, 2008, 10:49:44 PM
Remember you don't need to just press once. When I'm doing big beads I press in stages. I rarely fill all the corners on a first press even if the glass amount is perfect. I gently press once, to get the rough shape, then reheat and press again and it will look better. I can repeat this several times to get a nice even bead, without needing to press while it's too runny.

Never thought og that - thanks Mary!!

I hva a round tab press and I was making a footprint of the width and filling it in at first - but like others have mentioned on here - I now make it a bit smaller and barrel shaped and let the press gently push the glass to the ends!