Frit-Happens !

Lampwork => Common Problems => Topic started by: beads-on-toast on July 03, 2008, 08:10:22 PM

Title: is this propane? never happened b4
Post by: beads-on-toast on July 03, 2008, 08:10:22 PM
(http://i122.photobucket.com/albums/o262/beads-on-toast/burn.gif)

All these beads have the damage - what is it?
Title: Re: is this propane? never happened b4
Post by: fionaess on July 03, 2008, 10:54:45 PM
They look sooty... can you clean your torch jets?  That maybe the problem........ ???
Title: Re: is this propane? never happened b4
Post by: ♥♥Tan♥♥ on July 04, 2008, 03:09:23 PM
I get that when my propane is running low
Title: Re: is this propane? never happened b4
Post by: Funky Cow on July 04, 2008, 07:07:57 PM
I did too with my last tank
Title: Re: is this propane? never happened b4
Post by: Dwaa on July 07, 2008, 10:24:34 PM
Erm... whats up with them?