Lampwork => Lampworking Tip n Tricks => Topic started by: lemon kitten on June 24, 2008, 11:02:08 PM

Title: swirls
Post by: lemon kitten on June 24, 2008, 11:02:08 PM
OK......searched the website and can't find any reference to this.  What is the best way to make swirls.  I have sarted making beads with little tsunami type waves on them but I cant seem to get the blob to swirl.  I know I have to use a clear stringer, and I place it in the molten blob and twist but it just does'nt swirl the way I want it to.  I manged to do 1 out of about 10!! got any tips guys n gals?

Janey
Title: Re: swirls
Post by: catriona on June 24, 2008, 11:10:04 PM
Hi if you go to this link theres good tips i can now get lovely swirls http://www.frit-happens.co.uk/forum/index.php?topic=7004.0
xxcatxx
Title: Re: swirls
Post by: Redhotsal on June 24, 2008, 11:15:51 PM
Try using a really thick stringer.
Title: Re: swirls
Post by: lemon kitten on June 24, 2008, 11:17:45 PM
GREAT Tips!!! will try them tomorrow!

Janey x