Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: misspixie on June 19, 2008, 11:41:45 AM

Title: Murrini
Post by: misspixie on June 19, 2008, 11:41:45 AM
Ok... So, following Bev's wonderful tutorial in this months Bead & Beyond, I've made myself some murrini - very proud of myself too! Only forgot one thing... I've made this pretty stripy cane... And pulled the puntys off (can see the flower and everything!)... But I don't know what to cut it with! Will sharp wire cutters do it, or do I need something special?

Lucy x

(look! hehe)
(http://farm4.static.flickr.com/3023/2592680196_378b7af9a8_m.jpg)
Title: Re: Murrini
Post by: Jolene on June 19, 2008, 12:44:37 PM
Wow Lucy that is pretty. You can use rod nips (they look like big pliers but have a metal disk on each side) or I sometimes use nips that were originally for mosaic tiles to cut bits from the end of a rod
Title: Re: Murrini
Post by: LesleyMac on June 19, 2008, 01:52:08 PM
Or if you don't want to cut it, just heat the spot on the bead where you want it and push the end of  the rod  in and then cut it off with nips, you still have to cut but its easier to apply I find ;D
Title: Re: Murrini
Post by: misspixie on June 19, 2008, 01:57:11 PM
Thanks Jo :)

Right - off to buy myself some cutters then! ;D
Title: Re: Murrini
Post by: saffie on June 19, 2008, 02:06:08 PM
wow Lucy that is fab! well done you!
Title: Re: Murrini
Post by: turnedlight on June 19, 2008, 06:05:24 PM
That's lovely! I found Sarah Horniks tip handy, once you have pushed the murrini onto the bead, put a dot of clear on top to keep it looking good.. well, it worked for me anyway! :)
Title: Re: Murrini
Post by: Kaz on June 19, 2008, 07:57:18 PM
Really impressed with that - something that is on my list to try to learn how to do (when I have my next lesson!)
Kaz