Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Oxycon/Oxygen/Propane => Topic started by: Im a glassy babe on June 18, 2008, 08:50:18 PM

Title: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 08:50:18 PM
Hi there,

Can anyone help please?

Have a propane oxycon set up.  I keep finding that the propane gradually reduces when I'm beading.  We have checked for any leaks numorous times, and nothing appears.  I'm convinced it's something to do with the connection from the regulator to the propane bottle, but can find no evidence of a leak.

Help!!! It's really frustrating.  It does reduce slowly, but annoying nevertheless.

Any help appreciated

Thanks

Vicki
Title: Re: Propane Leak
Post by: Mary on June 18, 2008, 09:05:48 PM
Do you mean it's actually leaking, or is your pressure dropping? My pressure drops, it's just something my regulator does. I set it a little higher at the start now.
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 09:15:06 PM
Hi Mary

The regulator is set at maximum as per instructions from supplier.  We can't find a leak anywhere and have checked several times.  If I'm set at maximum will pressure drop gradually?  New to this so still learning.

Thanks

Vicki x
Title: Re: Propane Leak
Post by: Mary on June 18, 2008, 09:23:23 PM
It's hard to know without knowing your exact regulator,but if you can't find a leak that might be it.
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 09:28:58 PM
The complete kit to run your Hot Head Torch off bulk propane gas.
This kit enables you to run your Hot Head torch off a bulk cylinder of propane (LPG) gas. Although Mapp gas is the preferred gas for Hot Heads the costs soon start adding up as you get more hooked on beadmaking. Propane gas available from many garages, welding supplies, camp sites and garden centres is a close alternative to Mapp gas for your Hot Head although burning slightly lower in temperature this is not a major problem. Savings are huge by using propane as a normal 13 kilo cylinder will cost between £12 - £18.00 and will give 100 hours use. This kit contains a 4 bar  propane regulator, propane flashback arrestor, 5 mtr of propane hosing and the torch connector.All the kit is joined together and ready to use once you screw the cylinder on one end and the torch on the other.[/size]

Hi above is the description of regulator from website where I purchased.  Does this help at all?

Thanks
Title: Re: Propane Leak
Post by: Shirley on June 18, 2008, 09:34:10 PM
Hang on, you said propane oxycon set up, but you're using a hothead?
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 09:37:22 PM
No sorry, bit of confusion.

Started with a hothead when we purchased this hose and regulator.  Hubby then bought me a new torch and oxycon but am still using the same hose as used for the hothead.  Is this ok? We presumed as it was used for bulk propane with the hothead it was fine to carry on with the same hose when I changed set up.

have I got it all wrong?

Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 09:49:59 PM
If your regulator looks like mine (and it probabaly does, because your description is off Martin Tuffnell's website where I got mine) then the regulator is a bit hard to fathom! At first, I couldn't work out how to read the settings on the regulator, and didn't have it on the right setting. I moved from bulk propane to oxycon/propane setup too, and had to fiddle with the regulator while the torch was lit to make sure I had it right.
Title: Re: Propane Leak
Post by: Mary on June 18, 2008, 09:50:25 PM
You should be OK with the same bits. And a dual fuel needs less pressure than a HH, so the regulator should be OK. Are you maybe turning the dial the wrong way? Sorry to ask what seems obvious, but propane connections turn the "wrong" way, and I still sometimes close mine when I mean to open it.
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 09:54:50 PM
Thanks cathryn,

Is from Tuffnell's.  We were advised to open the regulator to maximum.  What kind of trouble were you having to fiddle with it?  Was it a problem with the flame? As new to this not sure what is supposed to happen when regulator is set at different pressures.

Thanks

Vicki x
Title: Re: Propane Leak
Post by: Redhotsal on June 18, 2008, 09:57:10 PM
You should be ok to use the same hoses. Try your regulator at "half way" - that is screw it all the way out and then count the number of screws needed to screw it totally in and then go back to half this number. That's about where I have mine. If you get down to gas bottle level you will see under the "tap" section of the regulator that there are two markings for min and max pressure. This IS a 0-4 bar variable regulator by the way? (looks like a great big black sink tap!)
I usually open the gas bottle only a little - probably no more than a turn and a half at the most.

How are you checking for leaks? By smell? Or by using a leak test solution. At a pinch you can use a spray of water with a few drops of detergent in it. If you liberally spray this all over the fittings you will see any leaks as little bubbles. This is really the best way to check. (By the way don't use this solution on your oxygen fittings - you really should used a proprietory leak detector fluid, which you can get from B+Qs) The leak detection fluid is simple and effective and tells you immediately if you have an actual leak or if you have pressure problems.
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 10:00:16 PM
Thanks Sally

Is maybe too much pressure causing this problem then?
Title: Re: Propane Leak
Post by: Redhotsal on June 18, 2008, 10:02:17 PM
Actually - reading back everything again I wonder whether you have the regulator set at fully closed rather than fully open? If so you will get some residual gas which is probably lurking in the hoses but the gas pressure will quickly drop and your flame will get tiny. It is confusing but I'm pretty sure "fully open" is actually "tap section screwed right in" on a propane regulator. Either way - I personally wouldn't have it fully open - half way and then adjust "to taste" is probably the best route...
Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 10:04:14 PM
Quote from: Redhotsal on June 18, 2008, 09:57:10 PM
I usually open the gas bottle only a little - probably no more than a turn and a half at the most.


Oooh - I open my gas bottle valve all the way  :-[  I set my regulator where I liked the flame  :-\
Title: Re: Propane Leak
Post by: Redhotsal on June 18, 2008, 10:08:00 PM
Well Cath, if it works for you that's fine. I guess you're relying on the regulator to control, well, actually regulate the gas flow - which is what it should be doing afterall. I've just always done it my way as no one ever told me any other way. As it seems to work I've never challenged it - coming from the University of "If it ain't Broke don't Fix it" as I am!  ;)
Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 10:11:03 PM
Sal, I was just glad to get over the sheer horror of the whole gas=massive explosion, run away quick while you're still alive syndrome  ;D 
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 10:16:11 PM
Thanks everyone,  will have a go tomorrow, and see if this improves it.

My husband has just sat and explained to me what a regulator is for.  I am a bit of a dizzy blonde.

If I've got it right.  If my propane is opened right out my regulator is passing through the maximum pressure to my torch.  If for some reason the pressure reduces in the tank it then reduces all along the line straight to my torch resulting in less propane.

If however, I have the pressure set at 2 bar for instance, then 2 bar will be fed to my torch.  If the pressure does drop in the tank, it won't affect the 2 bar pressure, unless the tank reduced below 2 bar, in which case what is after the regulator would reduce too.

Yay I think I get it!

Thanks
Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 10:20:11 PM
Of course, if your tank is running out, that plays merry hell with the pressure too  :o
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 10:24:51 PM
I wouldn't imagine it could be running out.  Have got a 19kg, (I know, prob a bit big) and I've had it since April.  Haven't had hours and hours on it, just manage to get some time in evenings and weekends, but worth a thought.

Thanks

Title: Re: Propane Leak
Post by: Redhotsal on June 18, 2008, 10:26:05 PM
Oh heck - now I'm really confused............. :-\
Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 10:26:30 PM
Get methodical tomorrow - you'll crack it  :)
Title: Re: Propane Leak
Post by: Funky Cow on June 18, 2008, 10:28:26 PM
Quote from: Redhotsal on June 18, 2008, 10:26:05 PM
Oh heck - now I'm really confused............. :-\


Welcome to my exclusive club, I'm the founder  ~ the permanently befuddled! It's free to join  ;D
Title: Re: Propane Leak
Post by: Redhotsal on June 18, 2008, 10:32:40 PM
Hehe - "get methodical" sounds like something out of Reservoir Dogs!
Title: Re: Propane Leak
Post by: Im a glassy babe on June 18, 2008, 10:40:43 PM
That last post from me prob made no sense what so ever, but I think I know what I mean!

My hubby reckons he did turn the regulator back in a half turn at one point, and I had told him it was a little better flame, so looks like this maybe the answer.  Great, we've been puzzling over this for a few days now.

Thanks again
Title: Re: Propane Leak
Post by: Im a glassy babe on June 19, 2008, 09:02:15 PM
Hi

Just me again getting a little more confused.

Well we adjusted the propane regulator and it did seem to improve.  I didn't have to adjust the propane for about half an hour.

Just wondering if it's usual to adjust after a while due to temperatures etc?

Anyone with any ideas?

Thanks

Vicki x
Title: Re: Propane Leak
Post by: julieHB on June 19, 2008, 11:33:05 PM
Hi, I might be totally off mark here, but according to what I have read, it is quite normal to have to adjust the torch dials until the torch is properly "worked in" (in lack of a more proper phrase).  I don't know which torch you have, but I have a couple of month old bobcat which has not been used that much, and I still have to turn up the propane (on the torch) after a bit of torching.  I just adjust the propane, keeping the oxygen constant, and off i go again - have never given it a second thought...do you think I should??  ;D
Title: Re: Propane Leak
Post by: Kaz on June 20, 2008, 08:01:57 AM
I have never given this much thought. I turn my propane tank full on - my DH set the regulator (not sure what to) and I constantly play around with the torch flame from when I first put it on as it always seems to drop a bit from that first surge.
Kaz
Title: Re: Propane Leak
Post by: turnedlight on June 20, 2008, 08:10:55 AM
I'm wondering if it's like mine - you turn it all on, and get a nice cone shaped flame, then start working, and after a little while, the flame goes bushy and you have to adjust the knobs on the torch? If that's it, then I'm getting it too, and I thought it was sort of normal, if a little annoying..
Title: Re: Propane Leak
Post by: dinah46 on June 20, 2008, 08:27:37 AM
I adjust my propane and oxygen all the time depending on what I am doing, oxygen down for reducing the silver glass, propane down to get a lovely little pinpoint flame, oxygen way up when I'm gettting impatient and it's not melting fast enough  ... now after reading this I'm wondering if I'm doing it all wrong ???
Title: Re: Propane Leak
Post by: Kaz on June 20, 2008, 08:29:48 AM
Quote from: dinah46 on June 20, 2008, 08:27:37 AM
I adjust my propane and oxygen all the time depending on what I am doing, oxygen down for reducing the silver glass, propane down to get a lovely little pinpoint flame, oxygen way up when I'm gettting impatient and it's not melting fast enough  ... now after reading this I'm wondering if I'm doing it all wrong ???
If so, then so am I....
Title: Re: Propane Leak
Post by: Redhotsal on June 20, 2008, 09:34:48 AM
It's probably the oxycon, not the propane. Once you've set your propane regulator you shouldn't have to keep changing it and if you're changing it as the oxycon changes you won't know if you're coming or going.

The oxycons are notorious for having a settling down period. One of mine settles in a minute or so but the other one takes a good ten minutes to sort itself out. Keep an eye on the little floating ball on the oxycon. If it's bobbing around then your flame will be all over the place. I try not to have my oxycons set at maximum output as they don't seem to like that. I run at about 4- 4.5 litres a minute.

When you first turn on the oxycon you WILL get a surge of oxygen after about 30 secs which is often enough to blow out the propane. This surge goes as quickly as it comes and then the oxygen starts to build up gradually as the internal oxycon reservoir fills. If you are changing your propane reg while all this is happening you will have all sorts of interesting flames! But by all means adjust the propane knob on the torch to suit.

Title: Re: Propane Reducing
Post by: Im a glassy babe on June 20, 2008, 11:11:40 AM
Quote from: julieHB on June 19, 2008, 11:33:05 PM
Hi, I might be totally off mark here, but according to what I have read, it is quite normal to have to adjust the torch dials until the torch is properly "worked in" (in lack of a more proper phrase).  I don't know which torch you have, but I have a couple of month old bobcat which has not been used that much, and I still have to turn up the propane (on the torch) after a bit of torching.  I just adjust the propane, keeping the oxygen constant, and off i go again - have never given it a second thought...do you think I should??  ;D

Thanks for that Julie,

Exactly the same torch as me, mine a couple of weeks old.  I do keep oxygen constant at 4.5 ltrs, but thought it strange to keep altering propane, but if that is what everyone does then great!  Was thinking that something was wrong along the way.  It has improved since we fiddled with the regulator, so can get about 1/2 hour before any adjusting (the torch that is, I'm not adjusting the regulator).  Does that sound about right according to yours?

Thanks Sally.  The oxycon seems steady to be honest.  I do watch the ball and doesn't seem to be bobbing about it definitely stays at 4.5 ltrs all the time, that's why I thought Propane problem. 

Looking back over the last few replies, a few of you seem to adjust regularly.  I just presumed once the torch was lit and steady, it would stay the same throughout the session.  I may be completely wrong.  When I did question this I was told it shouldn't need to be adjusted on the torch, but looks like many of you do.

Thanks everyone, looks like I'm maybe panicking over nothing then????

Vicki x
Title: Re: Propane Leak
Post by: julieHB on June 20, 2008, 01:58:22 PM
Ok, here's a quote from Corina tettinger's website, where she reviews several types of torches:

.....Con: While I love my GTT (Glass Torch Technologies, manufacturer, the two most adorable twins in the world, Willie and Wallie) torches, they have several "issues". In the first 6-8 month, depending on how much you work, the valves re-adjust themselves...I think it has to do with the material that is used, it expands for a while, until it's broken in. That means, you have to add propane or oxygen while you work, because the flame gets smaller and smaller.....

Does that reassure you?  It does me  ;D
Title: Re: Propane Leak
Post by: ThermalShock on June 20, 2008, 02:12:18 PM
Quote from: julieHB on June 20, 2008, 01:58:22 PM
Ok, here's a quote from Corina tettinger's website, where she reviews several types of torches:

.....Con: While I love my GTT (Glass Torch Technologies, manufacturer, the two most adorable twins in the world, Willie and Wallie) torches, they have several "issues". In the first 6-8 month, depending on how much you work, the valves re-adjust themselves...I think it has to do with the material that is used, it expands for a while, until it's broken in. That means, you have to add propane or oxygen while you work, because the flame gets smaller and smaller.....

Does that reassure you?  It does me  ;D


Well that certainly reassures me.  I bought my Bobcat at Towcester and I have to admit after I have lit the torch, after a few minutes (and continually every 10-15 minutes or so) I have to keep tweeking my propane knob as my flame has "shrunk".  Although annoying, I am not entirely sure there is anything that can be done about it.  My hubby assures me that our regulator etc... are all set correctly - and it didn't happen with my hothead, so I am guessing it was a Bobcat (or torches that have duel fuel) issue.  ::)
Title: Re: Propane Leak
Post by: Im a glassy babe on June 20, 2008, 03:43:04 PM
Quote from: julieHB on June 20, 2008, 01:58:22 PM
.....Con: While I love my GTT (Glass Torch Technologies, manufacturer, the two most adorable twins in the world, Willie and Wallie) torches, they have several "issues". In the first 6-8 month, depending on how much you work, the valves re-adjust themselves...I think it has to do with the material that is used, it expands for a while, until it's broken in. That means, you have to add propane or oxygen while you work, because the flame gets smaller and smaller.....

That's great, thanks for your help!  Does definitely reassure me.  I will take off my worry hat, and be putting the glass melting one back on!

Glad to know others with the bobcat do the same.

Thanks everyone!!
Title: Re: Propane Leak
Post by: dangerousbead on June 27, 2008, 04:37:31 PM
A massive THANK YOU to the lovely Mark,(Kaz's DH)  for the huge favour, won't say what it was here in case they all want it.
And no, there are no lines to read between here all you cheeky folks, it was glass and gas.
Title: Re: Propane Leak
Post by: Kaz on June 27, 2008, 05:53:23 PM
He says you're welcome and he quite enjoyed it really! ;)
Kaz
Title: Re: Propane Leak
Post by: Billie on June 27, 2008, 06:35:49 PM
OOooooooh!  I've seen the type of thing some people make with glass and gas  ;) :D :D :D :D