DOES NOT WORK
unless you want a dirty grey look...shall post a pic tomorrow - just wanted to let ya know
Yep clear on drk ivory is pants :D been there....got dissapointed :(. My very faves are clear over any of the ask colours, esp tirbal turq or berry creamy...yummy ;D
oooh got some tribal tourquoise will give it a go! ;)
ooo.... i got some clear frit knocking about.... must give that a go :)
Thanks for sharing Anna... :)
xx
Emma
Which clear frit do you mean over the ASK - I seem to have a couple of different ones? Would like to try this.
Kaz
Crystal clear. here's a picture.
http://www.beadenvy.co.uk/Photos/Bead%20Sets/pages/BS006.htm (http://www.beadenvy.co.uk/Photos/Bead%20Sets/pages/BS006.htm)
It makes a kind of lizzard/snake effect....cool ;D
That is cool - I'll have a play later on. Thanks :)
Kaz
According to Val Cox a lot of the furnace frits have lead in, which is why we can use them with other coe's, but lead reacts with ivory. If you can get 104 clear frit you'd probably be OK. Sorry, font of useless information me!
And we love you for it too Mary !!!!!!!!!!!!!!!!!!!!!!!!
;D ;D ;D
xxxxxxxxxxxxxxxxxxxxxxxxxxxx
I love clear frit over copper green - then etched, yum! ;D
Quote from: beadysam on June 12, 2008, 12:45:32 PM
I love clear frit over copper green - then etched, yum! ;D
you cheeky minx!!! i shall have to try this combo now - oh how you tease us so