Frit-Happens !

Lampwork => COE 104 => Topic started by: jewelchiz84 on June 05, 2008, 08:57:59 PM

Title: Black & White
Post by: jewelchiz84 on June 05, 2008, 08:57:59 PM
Right I need serious help (in more ways than one!).
I need to make some black and white beads, and im having a beeeeyatch of a time making them.
Everything I try is bleeding. Ive tried normal black effetre, but as we know thats actually purple, Intense black, and Hades. All tried with both normal effetre white and anice white. None of the combos are any good! Grrrrrrrrr! >:(
Anyone got any pics of black and white beads with no bleeding??
Anyone willing to let me know their secrets? Pleeeeeese!
I dont want to buy anymore glass unless I know its guaranteed to work.
Thanks people
~x~
Title: Re: Black & White
Post by: Shirley on June 05, 2008, 09:01:44 PM
Hades and peace, maybe? I can pop you a bit in the post - I owe you a thank you pressie :)
Title: Re: Black & White
Post by: turnedlight on June 05, 2008, 09:03:24 PM
Odd cotton is a nice white.. don't do much black and white though..
Title: Re: Black & White
Post by: jewelchiz84 on June 05, 2008, 09:04:46 PM
Hey Shirley
So that definatly works then?
That would be ace if you could! You know my addy dont you?
Title: Re: Black & White
Post by: jewelchiz84 on June 05, 2008, 09:06:28 PM
Is Odd Cotton an odd lot? or just the name? Ive never heard of that before
Title: Re: Black & White
Post by: MangoBeads on June 05, 2008, 09:07:02 PM
Quote from: Shirley on June 05, 2008, 09:01:44 PM
Hades and peace, maybe? I can pop you a bit in the post - I owe you a thank you pressie :)

Hades and Peace bleeds and spreads if over heated Effetre black and white works for me just dont over heat - Dont use anise white though as that has an organic side to it too .
Not very helpful but i used the effetre balck and white today with no problems.


Whoops realised its Vetro black I have !
Title: Re: Black & White
Post by: Vicki on June 05, 2008, 09:14:41 PM
these are vetro black & effetre white, I think i used intense to dot the flowers on, but I can't remember for sure, no bleeding from either anyway :)
(http://i49.photobucket.com/albums/f280/delica-girl/bw2.jpg)
Title: Re: Black & White
Post by: Josephine on June 05, 2008, 09:40:21 PM
Definitely vetro  black and effetre white. If you want a bit of the black to try PM me
Title: Re: Black & White
Post by: flowerjasper on June 05, 2008, 10:34:25 PM
sam does a fab frit called humbug, thats great, try that either left proud, melted in or swirled around,
sandy
Title: Re: Black & White
Post by: Lush! on June 05, 2008, 10:43:05 PM
I posted a black n white bracelet pic a couple of days ago with vetro black and effetre white - but I've just got some Hades and Peace today, I just had time to try one bead today - didn't notice any bleeding but I think my silver wire went brown and orrible on the Peace  :(

Title: Re: Black & White
Post by: jewelchiz84 on June 06, 2008, 09:41:43 AM
Thanks very much for all your suggestions. This has been driving me crazy for months!
~x~
Title: Re: Black & White
Post by: Shirley on June 06, 2008, 10:09:37 AM
I made a twisty with hades and black and then melted it in (lightly) onto a peace base and it didn't bleed.
I might have a rod of each in my car that might take a detour to Necton on the way home this afternoon! ;D
Title: Re: Black & White
Post by: glassworks on June 06, 2008, 10:22:27 AM
vetro black is a true black, and will not bleed or react... this can be good and bad i guess!  ;D ;D

hades is good, but a bit more pricey, and the very best will always be nero intense black hand made effetre - but it is the most expensive too...

Title: Re: Black & White
Post by: hatvary on June 06, 2008, 03:19:41 PM
What I have found is that if the base is black you'll have less bleeding than using a white base.
I had to make a set of beads with dots and stripes and the black based beads worked the best, what you also can do is make a white core encase this with clear and then put a black decoration on it. ;D