Hi there, can anyone tell me if there are any tricks to getting the beads of the mandrels without such a huge effort? I soak them in warm water the push the bead down whilst leaning on a chopping board. Any advice would be great, thanks ???
Title: Re: mandrel troubles
Post by: Kaz on May 30, 2008, 09:07:22 PM
Depends very much on the bead release you are using. If it is the stuff from the starter pack then it can (apparently) be like quick setting cement and you would probably do well to invest in some of the better bead release. I use Fusion from Martin and it works like a dream for me - as long as I keep it reasonably thinned down I rarely have to even use the pliers and can just twist the beads off by hand and I never soak them before removing the bead. Plus it makes the mandrels easier to clean for next time as all you have to do is wipe the remaining dry bead release off with a cloth or kitchen roll (being careful of course not to inhale the dust).
Kaz
Title: Re: mandrel troubles
Post by: turquoise on May 30, 2008, 09:21:00 PM
yes I have got the same stuff. I think it is way too think then, it is a real nightmare. I will try thinning it down with a bit of water ;D and see if that does the trick. Thank you.
Title: Re: mandrel troubles
Post by: garishglobes on May 30, 2008, 09:23:09 PM
I'm using Foster Fire at the moment and rarely have to resort to pliers. It is great!
I believe soaking in vinegar can help if you really have a stuck bead - overnight if it is really stuck. If it is still stuck, I would usually reckon on it being absolutely bent on being a mandrel decoration and leave it to it.
If you have just started though, the other thing to watch out for is how hot you are getting your beads. Very hot (gloopy hot) can also cause beads to stick more than usual.
Title: Re: mandrel troubles
Post by: Sulis (Hazel) on May 30, 2008, 09:44:04 PM
Hi Turquoise,

For moderately stuck beads I tend to put the other end of the mandrel in a bench vice, keeping it upright. Hold the bead tightly and begin to twist the bead gently but firmly from side to side until it starts to give a little. keep doing that until it frees itself and you should then be able to pull it up off the mandrel.

For more firmly stuck beads, I have heard that some people put the mandrel and bead in ice (or the freezer) for a little while, which I'm told causes the steel to contract slightly and therefore can free the bead - however I haven't tried that yet.

If all else fails, learn to love your decorated mandrel, tie a tag to it and use it to mark where you've planted something nice in the garden  ;)

I'm a fan of the flame dry Fusion bead release from Martin, (a recent convert) - but I thin it with water until the consistency of single cream before use and mix it like heck!

Good luck  :)
Title: Re: mandrel troubles
Post by: TiaraHelen on May 30, 2008, 09:56:29 PM
I've been twisting mine off holding the mandrel with pliers, and only one ever stuck (I just broke it off to save the mandrel, as the bead was rubbish).  I have noticed that sometimes twisting the bead further ONTO the mandrel instead of trying to pull it off can help get the bead moving.

Hx
Title: Re: mandrel troubles
Post by: June on May 30, 2008, 10:55:01 PM
We like FosterFire and rarely have stuck beads  ;D 
Title: Re: mandrel troubles
Post by: firedinglass on May 30, 2008, 11:11:51 PM
I add a little bit of washing up liquid to the warm water to soak mandrels, i also rub the release off right up to bead before i soak. If it's really stuck flat coke usually get's it off! good luck, there will sometimes  be one stubborn one that won't shift....
Title: Re: mandrel troubles
Post by: turquoise on May 31, 2008, 11:50:24 AM
lots of advice there thanks everyone. I will definately thin my bead release with a dash of water and also dig out some pliers. As for flat coke sounds good, it is also very good for cleaning the loo!!!
Title: Re: mandrel troubles
Post by: Les on May 31, 2008, 11:53:18 AM
Quote from: turquoise on May 31, 2008, 11:50:24 AM
As for flat coke sounds good, it is also very good for cleaning the loo!!!

And people STILL drink this stuff ?? ??? ??

LOL

xxx
Title: Re: mandrel troubles
Post by: Amber on May 31, 2008, 01:12:43 PM
What everyone else said...and if it's really stuck, a squirt of WD40 often does the trick!  :)
Title: Re: mandrel troubles
Post by: June on May 31, 2008, 01:26:14 PM
I've also seen somewhere that neat toilet liquid (ie toilet duck) was good, but not tried it myself ?
Title: Re: mandrel troubles
Post by: garishglobes on May 31, 2008, 07:02:45 PM
Well that kind of makes sense, if flat coke cleans the loo well.. reversing this, I wonder what fizzy toilet duck is like?
Title: Re: mandrel troubles
Post by: Shirley on May 31, 2008, 07:52:19 PM
Quote from: garishglobes on May 31, 2008, 07:02:45 PM
Well that kind of makes sense, if flat coke cleans the loo well.. reversing this, I wonder what fizzy toilet duck is like?

I don't know, but I wouldn't try drinking it! :D
Title: Re: mandrel troubles
Post by: June on May 31, 2008, 09:14:52 PM
LOL !!  ;D ;D
Title: Re: mandrel troubles
Post by: mad bunny on June 01, 2008, 10:21:13 AM
I usually have to twist off with pliers. 
So I will try and thin down my bead release.  thanks everyone