Title: how am i burning the glass!!
Post by: flowerjasper on May 11, 2008, 09:35:20 PM
hi,
not sure what i am doing wrong, a couple of things keep happening and its making me a tad peed off!!
i am on a hothead on bulk,
if i use clear frit it goes silver! i want that "fruit pastille sugar effect"
a lot of the frit i use goes brown/ grey (not just on ivory),
today i used mint sparkle on clear , the clear looked yellowy and i couldnt see the mint!(i know this combo looks fab  as i hve some Lush! beads)
when i encase i get brown streaks in the clear.
all of what i do is hit and miss, the tips fom here have been a great help
any ideas? am i over heating the glass?
sandy
Title: Re: how am i burning the glass!!
Post by: ♥♥Tan♥♥ on May 11, 2008, 09:38:50 PM
aha your flame is too reducing, its too bushy and that is what is making all of your glass mucky, it may well be that you are working too far down in the flame, try a rod of yellow and hold it in the flame, if it goes mucky pull the mucky bit off and try again further up, keep doing this until its not mucky anymore and thats where you need to work in the flame.

If that doesnt work then you need to cover the holes around the base of your hot head with some tin foil
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 11, 2008, 09:47:23 PM
will try that tomorow tan,
i thought if i covered the holes up thats what gave a reducing flame, another thing  ive got wrong!!
i just turn the hothead on, could it be that i am yurning it up too high??
Title: Re: how am i burning the glass!!
Post by: ♥♥Tan♥♥ on May 11, 2008, 09:58:35 PM
ooo dont quote me on the covering the holes then, its been a long time since I was on a hot head, but try the yellow glass thing too, it picks up smut quickly but is cheaper than trying it with pink ;D
Title: Re: how am i burning the glass!!
Post by: garishglobes on May 11, 2008, 10:36:59 PM
Definitely don't cover the holes!! It'll make things more reducing for sure. The yellow glass thing is a good idea though.
If this has only just started happening, you could have a bad lot of propane (some seems to be "dirtier" than others, for no good reason) or possibly a mucky hose? Easiest to start with experimenting with working position though, and go from there...
Title: Re: how am i burning the glass!!
Post by: julieHB on May 11, 2008, 10:39:51 PM
Also, could it be that the propane cylinder is nearly empty?  I've read somewhere it might be more yucky then.
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 11, 2008, 11:12:49 PM
thanks, i will work further out, and try the yelow rod thing,
its so frustrating when the frit is lovely in the pot and poo on my beads!!
could be the propane is running out, is there maintence that should be done on a hot head? 
dirty hoses? would i just wash them out ? ???
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 11, 2008, 11:45:06 PM
does the angle of the torch matter?
i have noticed that mine is at a different angle to everyone elses  ::)
(http://i251.photobucket.com/albums/gg313/flowerjasper/lushbracelet006.jpg)
Title: Re: how am i burning the glass!!
Post by: Redhotsal on May 11, 2008, 11:59:03 PM
I like your spotty pinny...... ;)
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 12, 2008, 07:39:57 AM
thats my dog grooming top, so lovely to wear nylon in the hot weather!!
it has paws all over it  ;D
Title: Re: how am i burning the glass!!
Post by: Amber on May 12, 2008, 10:36:05 AM
My torch is at the same angle as yours and it seems to be fine...

I started getting burn marks when I was right at the end of my propane, that can definitely do it. Also might be worth checking whether there are any 'bits' (glass, bead release...) in the torch itself.
Title: Re: how am i burning the glass!!
Post by: Shirley on May 12, 2008, 10:59:42 AM
I'd say it's mucky propane. I've been making a lot of beads with black nebula recently and getting a good reduction. Made a great tube bead on Saturday but couldn't get the reduction at all, just sooty marks. The tank is definitely on its last legs so I'm pretty sure that's what it is in my case.
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 12, 2008, 12:07:46 PM
i hope its that!!
would be a sad life if i could never have clear clear  :D
was thinking it was me  :D
Title: Re: how am i burning the glass!!
Post by: June on May 12, 2008, 05:53:00 PM
Sandy, I had that a lot with my HH, especially with clear and pale transparents.  If the tips about the propane don't solve your problem, you may need to work further up in the flame and then be patient (something I sadly lack, hence the reason I didn't do a lot of encasing  !) 
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 12, 2008, 11:04:42 PM
took your advice ladies , worked further up the flame and managed to keep a bit if clear frit clear, i also encased ( wonkily!) and the clear wasnt so streaked, 
i think the propane is coming to the end as well,  ::)
ta all x
Title: Re: how am i burning the glass!!
Post by: mindy23 on May 29, 2008, 11:04:26 PM
I have the similar trouble when the propane is nearly finished.  Also, its a good idea to make sure that your rods are super clean before you use them as any bits or dust or even just oil from your fingers can make horrible cloudy bits.  I clean mine with meths before I'm going to use them.  Its especially important with the transparent ones. 

Mindyx
Title: Re: how am i burning the glass!!
Post by: flowerjasper on May 29, 2008, 11:10:43 PM
its becoming clearer to me now that the fact i groom dogs in the same space i lampwork does have certain effects!!
dust, dog hair ( for ages i was puzzled by the wiggly black lines on beads i had put in vermiculite...)
so i will work further up the flame, keep the vermiculite out of the shed whilst i am grooming, especially like tonight, the hairiest golden retriever, hair every where.... wiggly lines for a week me thinks!!
Title: Re: how am i burning the glass!!
Post by: mindy23 on May 29, 2008, 11:26:47 PM
LOL!!

I have a deerhound, (long grey hair), a wirey mongrel ( wirey black hair) and a black greyhound, there seems to be nothing that their hair doesnt stick too.  I have all the ahir bases covered I think.  I should plan better when getting my dogs I think.  All one colour maybe so I can get a carpet and furntiure that hides it better!!! ;D
Title: Re: how am i burning the glass!!
Post by: biccy99 on May 30, 2008, 12:19:16 PM
Yeah my ginger cat doesn't go well with my black clothes (or beadmaking lol)