Frit-Happens !

Lampwork => COE 104 => Topic started by: Rachel B on April 07, 2008, 02:30:24 PM

Title: Dark Silver Plum
Post by: Rachel B on April 07, 2008, 02:30:24 PM
Can anyone let me know what other glasses look fab when used with DSP, I want to experiment but then I don`t want to be wasteful with my precious glass.  Pics would be fab too.  Ta you wonderful glassy peeps! ;D
Title: Re: Dark Silver Plum
Post by: Shirley on April 07, 2008, 05:04:33 PM
I tried it over ivory - dots and stringers and it went a great bronzey colour
Title: Re: Dark Silver Plum
Post by: ebj on April 07, 2008, 08:07:12 PM
Really not very exciting but here is a pic of it with Vetrofond Ivory ( I think -I made this an AGE ago). The silver plum dosent react  with the ivory the same as it does moretti ivory. I'm sure I made more with this colour combo - If I can find any pics I'll edit this post and bung them up :) Just dont laugh at my boring beads lol!


(http://i18.photobucket.com/albums/b114/emmabaird/Jewellery/CIMG6016.jpg)
Title: Re: Dark Silver Plum
Post by: June on April 07, 2008, 08:08:58 PM
I like it and it looks great with that silver necklace  ;D
Title: Re: Dark Silver Plum
Post by: ebj on April 07, 2008, 08:13:17 PM
its a bracelet lol :) But thanks, it was a gift for my grandma. She still dosent understand I dont think that I "MADE" the bead lol!  ::) 
Title: Re: Dark Silver Plum
Post by: June on April 07, 2008, 08:14:58 PM
LOL - yes, now I've looked again, it would probably bit a tad too tight round the neck !   ;D
Title: Re: Dark Silver Plum
Post by: Dragonfire Glass on April 07, 2008, 09:44:04 PM
DSP on light sky blue

(http://i169.photobucket.com/albums/u211/df-glass/focals/B293.jpg)
Title: Re: Dark Silver Plum
Post by: Sherry Bellamy on April 07, 2008, 10:21:23 PM
Thin, fine, slightly raised scrollwork in DSP looks fantastic on the pale transparents, especially the pale browns like 049 and 018.  I did a set a long time ago that was just assorted pale lentils with DSP scrolls that I melted in a wee bit, they were really pretty. Don't know if I have a pic, though. I'll look just as soon as I finish the set from hell that I'm currently making.
Title: Re: Dark Silver Plum
Post by: Rachel B on April 08, 2008, 08:25:44 AM
Thank you, I`ll go and dip some mandrels and go and play!