Lampwork => COE 104 => Topic started by: Donna@Rockin' Beads on March 15, 2008, 03:31:00 PM

Title: Muddy Transparent Glass all of a sudden
Post by: Donna@Rockin' Beads on March 15, 2008, 03:31:00 PM
My transparent glass and quite a few of my frits seem to have gone all yucky all of a sudden. Could it possibly be because my bottle of propane is nearing the end (I've been using it more or less for 5-7 hours every week since October last year and I can't hear any sloshing in it any more). The muddiness appeared about 3 weeks ago and is affecting all types of transparent glass and some of the frit mixes.
Could it be a near empty bottle of propane or something else?
I am on a Minor with an Oxycon and big bottle of propane and haven't changed anything (I think!!!).

Thanks guys......
Title: Re: Muddy Transparent Glass all of a sudden
Post by: Kay on March 15, 2008, 03:52:02 PM
someone posted about this a few weeks back. They were coming to the end of their bottle too
Title: Re: Muddy Transparent Glass all of a sudden
Post by: Donna@Rockin' Beads on March 15, 2008, 03:53:58 PM
Thanks, I'll have a hunt for the thread, although a search on propane brought up quite a few hits last time, as I'm sure you can imagine!!!  ;D
Title: Re: Muddy Transparent Glass all of a sudden
Post by: Donna@Rockin' Beads on March 15, 2008, 03:56:28 PM
Right, I've found the thread and now know for sure that I need to get a new tank.
That was easy.....
Title: Re: Muddy Transparent Glass all of a sudden
Post by: Kay on March 15, 2008, 03:58:47 PM
its lasted a fair while Donna, glad you found the thread, I searched but couldnt find it