Frit-Happens !

Lampwork => Common Problems => Topic started by: TALIZMAN on February 18, 2008, 12:59:47 PM

Title: hollow rods
Post by: TALIZMAN on February 18, 2008, 12:59:47 PM
I saw some of these at kaz's place at the weekend, but didn't really know for what purpose they were intended.... just like a tube of glass really....?
Title: Re: hollow rods
Post by: *rowanberry* on February 18, 2008, 01:10:29 PM
did it have a pearlescent sheen to it? is so that is seeded glass and is very special and lovely and goes all bubbly!

If not it might just be glass tubing which can be used for all different funky things, bottles and vessels! I am after some 104 tubes at the mo...
Title: Re: hollow rods
Post by: Kaz on February 18, 2008, 01:22:19 PM
It is seeded glass - there were just 2 rods and I have both of them as no-one took them (evil laugh ;D). I made a little pair of beads yesterday and they are really cute - like tizer in a bead!!! Where can we get more???
Kaz
Title: Re: hollow rods
Post by: *rowanberry* on February 18, 2008, 01:26:36 PM
I so LOVE seeded glass! I am after some more actually myself - totally obsessed with it! The only place I can find it is http://www.morettiandmore.net

In answer to your question Heidi,
it does this rather special bubbly effect and is lovely on a dark background:
(http://farm3.static.flickr.com/2319/2165388037_54f3443c2c_o.jpg)
Title: Re: hollow rods
Post by: June on February 18, 2008, 01:42:48 PM
They're rather nice, Claire !   ;D ;D
Title: Re: hollow rods
Post by: garishglobes on February 18, 2008, 01:44:58 PM
They're lovely.
There was some on ebay a couple of days ago, but listing is now ended - don't know if seller has more..
Title: Re: hollow rods
Post by: Kaz on February 18, 2008, 01:45:50 PM
Looks very interesting Claire - if you are doing a Moretti and More order before Towcester let me know and I could then add some stuff and share the postage/customs and collect from you then?
Kaz
Title: Re: hollow rods
Post by: glassworks on February 18, 2008, 01:53:27 PM
i have about 6 colours here - we have a limited stck so we have not listed them.. i have a big order going into effetre today or tomorrow if anyone wants to let me know if there is demand for this?.. bear in mind i have to buy at least 22lb's per colour!!..

;D
Title: Re: hollow rods
Post by: Kaz on February 18, 2008, 02:04:22 PM
Q - I wouldn't want 22lbs but I am certainly interested  ;D - I liked the effect and it was quite easy to work. (You see I was in daring mode yesterday!) How much is it? Is it possible to put a mixed pack - say 2 rods of each colour to one side for me - I will be ordering some stuff (opalinos) after payday!
Kaz
Title: Re: hollow rods
Post by: TALIZMAN on February 18, 2008, 02:40:57 PM
hmmm - that looks nice.....! I like it!!!

I'm going to my "class" this coming weekend and then I'll be home I think to turn my HH on (for the 2nd time.....) I think i've played now on more 'proper' torches than my own!! hehehehe (evil cackle).

My dad told me ages ago about an oxycon that he knew someone (who had died) had.... I told him to get it if he could.... just spoke to him before and it went in the skip!!!!! (he wasn't quick enough and this guys family just had a mass clearout!) Aaaargh!
Title: Re: hollow rods
Post by: glassworks on February 18, 2008, 02:41:22 PM
yep, we can do mixed packs of a few rods of each colour, up to say 250gms?..

8)
Title: Re: hollow rods
Post by: GoodMonkey on February 18, 2008, 02:49:31 PM
Quote from: glassworks on February 18, 2008, 02:41:22 PM
yep, we can do mixed packs of a few rods of each colour, up to say 250gms?..

8)


I would like a mixed pack too.  Do you have it in stock now?  I am putting an order in with you this evening.
Title: Re: hollow rods
Post by: Sal on February 18, 2008, 02:53:49 PM
Wow Claire-they are gorgeous! One day, when I have money (haha!) I'd love to have a go with some of this  ;D
Title: Re: hollow rods
Post by: ♥♥Tan♥♥ on February 18, 2008, 02:56:46 PM
It is fantastic glass to work with but beware its shocky as hell so go slowly to begin with and its a dream ;D
Title: Re: hollow rods
Post by: *rowanberry* on February 18, 2008, 03:45:30 PM
Tan is right, its a right shocky little glass - and a booby-burn risk!  :-[  ::) But start slow and melt slowly and its okay, possibly pre-warm.

Q, i'd be interested if you stocked this - it's actually my most favourite glass!!! I'd happily get a lot in one go, depending on cost. 1/2 - 1kilo of the aqua and 1/4kilo of each of the other colours.

If you had any in stock at the mo, even a few rods that we could order in time for sundays meet that would be good :D

Heidi! OMG! an oxycon in the skip! nooooooooooooooooooo! Hell if you got that I could have even leant you my spare minor burner until you got your own!
Title: Re: hollow rods
Post by: beadysam on February 18, 2008, 03:47:47 PM
I luurve seeded glass its yummy!   ;D
Title: Re: hollow rods
Post by: Billie on February 18, 2008, 04:01:03 PM
I'm coming to see you Wednesday Q (if you're home)... save me some pleeeeeeeeeeeeeease!!
Title: Re: hollow rods
Post by: Maikki on February 18, 2008, 05:16:23 PM
I am interested too...
Title: Re: hollow rods
Post by: turnedlight on February 18, 2008, 05:19:11 PM
I'm interested..
Title: Re: hollow rods
Post by: glassworks on February 18, 2008, 05:26:55 PM
oh hell....

8) ;D ;D ;D
Title: Re: hollow rods
Post by: *rowanberry* on February 18, 2008, 05:28:20 PM
I think seeded glass looks like its going to be popular! LOL!

Anyone ever seen Tink Martins vessels with it? YUMMY!!!!!!!
Title: Re: hollow rods
Post by: Maikki on February 18, 2008, 05:37:16 PM
I was actually reading Sarah HornikĀ“s blog this weekend and she had beads made from it. OT: It was so nice to read the blog from the very beginning to the current entrys and see how her style have developed. 
Title: Re: hollow rods
Post by: Lush! on February 18, 2008, 06:48:27 PM
Quote from: *rowanberry* on February 18, 2008, 03:45:30 PM- and a booby-burn risk! 

I was proudly showing off my booby burns today  ;D ;D

Title: Re: hollow rods
Post by: Kaz on February 18, 2008, 08:10:22 PM
Quote from: TALIZMAN on February 18, 2008, 02:40:57 PM
hmmm - that looks nice.....! I like it!!!

I'm going to my "class" this coming weekend and then I'll be home I think to turn my HH on (for the 2nd time.....) I think i've played now on more 'proper' torches than my own!! hehehehe (evil cackle).

My dad told me ages ago about an oxycon that he knew someone (who had died) had.... I told him to get it if he could.... just spoke to him before and it went in the skip!!!!! (he wasn't quick enough and this guys family just had a mass clearout!) Aaaargh!
Just got visions of the cooked hand gang hanging round outside old people's homes and sheltered housing in case someone on oxygen pegs it :o
Kaz
Title: Re: hollow rods
Post by: Vicki on February 18, 2008, 08:55:19 PM
I wondered what seeded glass was...I want some too ;D
Title: Re: hollow rods
Post by: Kaz on February 18, 2008, 08:59:42 PM
Quote from: glassworks on February 18, 2008, 02:41:22 PM
yep, we can do mixed packs of a few rods of each colour, up to say 250gms?..

8)
Yes, please Q - could you definitely put a 250g pack to one side for me - I will be ordering other stuff after the end of the month. (p.s. how expensive is it???)
Cheers
Kaz
Title: Re: hollow rods
Post by: saffie on February 18, 2008, 09:00:06 PM
Quote from: cheekycherubbeads on February 18, 2008, 08:10:22 PM
Quote from: TALIZMAN on February 18, 2008, 02:40:57 PM
hmmm - that looks nice.....! I like it!!!

I'm going to my "class" this coming weekend and then I'll be home I think to turn my HH on (for the 2nd time.....) I think i've played now on more 'proper' torches than my own!! hehehehe (evil cackle).

My dad told me ages ago about an oxycon that he knew someone (who had died) had.... I told him to get it if he could.... just spoke to him before and it went in the skip!!!!! (he wasn't quick enough and this guys family just had a mass clearout!) Aaaargh!
Just got visions of the cooked hand gang hanging round outside old people's homes and sheltered housing in case someone on oxygen pegs it :o
Kaz

this had me in absolute stitches, brought out the nursing sense of humour that i have i can just picture it now!!!! ROFL  ;D   ;D  ;D   ;D  ;D  ;D  ;D
Title: Re: hollow rods
Post by: TALIZMAN on February 20, 2008, 11:04:36 AM
hahaha - this has made me giggle... I think these nursing homes better watch out..!
Title: Re: hollow rods
Post by: Dragonfire Glass on February 20, 2008, 12:24:03 PM
I don't see any mention of price  :)

Gone are the days when I say yes I'll have it, only to find out I couldn't afford it!
Title: Re: hollow rods
Post by: Kaz on February 20, 2008, 12:29:32 PM
Yes it was a bit of an afterthought to ask and since then a massive silence from Q on that issue!!!! ;D
Kaz
Title: Re: hollow rods
Post by: Stacy on February 20, 2008, 01:06:15 PM
mmmmm - these look lovely - I would also be on the interested list!!!
Title: Re: hollow rods
Post by: dangerousbead on February 20, 2008, 01:15:44 PM
I'd be interested in a rod or two of the seeded glass, how would it be if we put a bulk order in through one of us and sort it out at the next get together? Or is that too complicated?

Kaz "Cooked HAnd GAng"   :D ;D :D ;D :D   I love it !   Maybe that could be our collective name.
Title: Re: hollow rods
Post by: dinah46 on February 20, 2008, 01:18:42 PM
Quote from: dangerousbead on February 20, 2008, 01:15:44 PM
I'd be interested in a rod or two of the seeded glass, how would it be if we put a bulk order in through one of us and sort it out at the next get together? Or is that too complicated?

Kaz "Cooked HAnd GAng"   :D ;D :D ;D :D   I love it !   Maybe that could be our collective name.

I think that sounds a good idea, I could wait until April
Title: Re: hollow rods
Post by: Jolanda on February 20, 2008, 02:25:05 PM
Quote from: *rowanberry* on February 18, 2008, 01:10:29 PMIf not it might just be glass tubing which can be used for all different funky things, bottles and vessels! I am after some 104 tubes at the mo...

Would you tell us when/if you find those, please... I am looking for some 104 tubing to make balls with...
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 02:54:33 PM
I found these:
http://www.howacoglasssupplycompany.com/glaskolben_tubes.html
These are sealed end thingummies but look interesting!

(howaco is ace btw! I just bought black nebula & green envy from her sooo cheap and the shipping was hardly anything!)
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 03:01:20 PM
Lauscha also does tubing I know, but its a pig to find someone stocking it!
Title: Re: hollow rods
Post by: TALIZMAN on February 20, 2008, 03:03:50 PM
oh to win the lottery eh!!?
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 03:11:27 PM
Just found this on tubing too...
http://www.wetcanvas.com/forums/archive/index.php/t-121138.html
Title: Re: hollow rods
Post by: Kaz on February 20, 2008, 03:31:28 PM
howaco looks a really good site - their price for stringer is excellent as well. I will be ordering I think......
Kaz
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 04:08:14 PM
I bought all of my tools etc from them when I started. They are my fave US supplier. I fancy some of their glow frit next :D
Title: Re: hollow rods
Post by: TALIZMAN on February 20, 2008, 04:13:02 PM
glow frit?

is that like glow in the dark - cos that WOULD be cool
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 04:16:36 PM
It certainly is!!!!! Imagine how cool a night sky bead would be with that :D
Title: Re: hollow rods
Post by: glassworks on February 20, 2008, 04:50:10 PM
we'll make up some mixed packs and stick them on the shop.. and i have a fair supply of lauscha tube, thin wall only and about 10-15mm diam?..   ;D ;D
Title: Re: hollow rods
Post by: *rowanberry* on February 20, 2008, 05:00:33 PM
Any time we need to order by tonight Q to get it in time for the bash on Sunday? I sure want some of that there tubing... both seeded and lauscha...

I've been reading up on soda lime glass tubing today actually, seems that Schott do a range of tubing in 90coe & anneals at 530c (ie compatible with Bullseye) tubing in different diameters and thicknesses and say its suitable for artistic applications & xmas decorations. Its Schott's AR-Glass range.... now to find someone who stocks it in sensible quantities, and at a price I can afford.
Title: Re: hollow rods
Post by: Revontulet on February 20, 2008, 06:49:46 PM
Quote from: glassworks on February 20, 2008, 04:50:10 PM
we'll make up some mixed packs and stick them on the shop.. and i have a fair supply of lauscha tube, thin wall only and about 10-15mm diam?..   ;D ;D

Are they there yet...... ;D
Title: Re: hollow rods
Post by: TALIZMAN on February 20, 2008, 08:29:09 PM
Quote from: *rowanberry* on February 20, 2008, 04:16:36 PM
It certainly is!!!!! Imagine how cool a night sky bead would be with that :D

I so NEED a bead that glows in the dark!!!!!! just one (she says!)... plain round one to go on a choker with glow in the dark frit on it..... ;D
Title: Re: hollow rods
Post by: Black Heart Beads on February 21, 2008, 12:55:21 AM
Quote from: TALIZMAN on February 20, 2008, 08:29:09 PM

I so NEED a bead that glows in the dark!!!!!! just one (she says!)... plain round one to go on a choker with glow in the dark frit on it..... ;D

I ordered a couple of bags of glow in the dark frit from the US weeks ago. It was one of those middle of the night buys, don't think I will use much just want to give it a go. When it does eventually get to me I will pop a little in the post to you.
Title: Re: hollow rods
Post by: Maikki on February 21, 2008, 07:21:38 AM
Poledra has glow in the dark powder and we tested it a little some time ago. I tried just once and found out it was a bit tricky - burned easily etc. Then you had to have it outside to collect light/energy/something from sun and after that it glowed in dark some time. I do not know if the frit is same stuff and if it is easier, because there are more material in it I guess.
Title: Re: hollow rods
Post by: Juniper on February 21, 2008, 07:40:46 AM
Quote from: Maikki on February 21, 2008, 07:21:38 AM
Poledra has glow in the dark powder and we tested it a little some time ago. I tried just once and found out it was a bit tricky - burned easily etc. Then you had to have it outside to collect light/energy/something from sun and after that it glowed in dark some time. I do not know if the frit is same stuff and if it is easier, because there are more material in it I guess.

;D I have a habit of collecting shiny things!  ;D ;D ;D
Title: Re: hollow rods
Post by: TALIZMAN on February 21, 2008, 10:58:29 AM
Quote from: samantha on February 21, 2008, 12:55:21 AM
Quote from: TALIZMAN on February 20, 2008, 08:29:09 PM

I so NEED a bead that glows in the dark!!!!!! just one (she says!)... plain round one to go on a choker with glow in the dark frit on it..... ;D

I ordered a couple of bags of glow in the dark frit from the US weeks ago. It was one of those middle of the night buys, don't think I will use much just want to give it a go. When it does eventually get to me I will pop a little in the post to you.

ooooh!! :-*
Title: Re: hollow rods
Post by: flowerjasper on February 23, 2008, 12:28:39 AM
just looked for the seeded glass rods on Q`s site,
cant find them,
put in seeded glass in search and nothing,
will try again tomorrow,
sandy
Title: Re: hollow rods
Post by: Billie on February 23, 2008, 07:12:10 AM
PM him.  Q had some mixed sample packs while I was there Wednesday... (although that's not to say he hasn't sold it all!)