Frit-Happens !

Lampwork => Common Problems => Topic started by: fionaess on February 09, 2008, 02:55:42 PM

Title: Encasing
Post by: fionaess on February 09, 2008, 02:55:42 PM
I am totally, utterly useless at this...  I have made 3 lovely beads.. encased them and ended up pulling them into stringers.. I hate, detest, loath encasing.. I am never, ever ever going to try to encase anything ever again, I am going to be know over land and sea as the non encasing lampworker... I promise faithfully never to attempt to encase anything ever again  .. well probably until Wednesday !!!
Phewww... I needed to get that of my chest..... I have spent abot 3 hours trying to do this,, it is/I am hopeless... 3 hours on 3 lots of ugly stringer... poooooo !!!!!


Fiona
Title: Re: Encasing
Post by: Funky Cow on February 09, 2008, 03:15:50 PM
Ooooooooooooooooooooooooooh my friend - I really do know how you feel! But fear not, if ham-fisted me can get the hang of it - there is hope for everyone. Try this
http://www.kikibead.com/techniques/casing.htm (http://www.kikibead.com/techniques/casing.htm)
and you will see that when you heat one side of the bead, the encasing glass really does 'pull' over. The knack is getting the right amount of encasing glass on, and I usually marver mine gently to make it a kind of 'belt' around the middle of the bead before heating each end in turn Give it go, and report back please  ;)

Cath x
Title: Re: Encasing
Post by: afina on February 09, 2008, 03:18:08 PM
Hi Fiona,
encasing is difficult in the beginning. Just don't give up! I so do remember my fist "encased" beads, they were sooo ugly! Then it got better, and suddenly it just worked! It is only PPP.  But I wouldn't pull the beads into stringers, I would finish them as they are and later look at them so to see what should be done in a different way.
You'll manage, as long as you don't give up.  8)
Title: Re: Encasing
Post by: fionaess on February 09, 2008, 03:50:38 PM
If you had spent 30 mins trying to melt a huge blob of effetre clear into a round bead.. and being so careful not to burn the damn stuff, and still ended up with a huge blob of clear.. you too would cut your losses and pull the damn thing into stringers   :D :D :D :D

Fiona
Title: Re: Encasing
Post by: Shirley on February 09, 2008, 03:56:19 PM
I think the point is, we haveall done exactly that, but have stuck with it and it does get easier as you get more used to how the glass works. Give it a rest for a bit, then go back to it, and you will find it gets a little better each time. :)
Title: Re: Encasing
Post by: ♥♥Tan♥♥ on February 09, 2008, 04:04:11 PM
Take a little plain bead, about the size of a pea, run a wrap of clear around it......you have encased something.

Make another plain bead, put some dots around it, melt them in, let it cool to tapping coolness, i.e tap it on your marver, if it taps its cool enough, wrap a layer of clear round it melt it in....thats encasing decoration

Now look at them, you have encased a plain bead and a decorated bead, both very simple, the edges are bleeding around the mandrel, but you have encased.

Now do the same with a small barrel bead but wrap clear around both ends and a little bit around the centre if you need it.

And again with a dotty decorated barrel.

Keep it small, keep the practice on beads that dont matter
Title: Re: Encasing
Post by: Sal on February 09, 2008, 04:11:13 PM
Encasing seems to be one of those things you're rubbish at for ages, feel like you're never going to be able to do it then suddenly one day you get it. I'm by no means an expert but my encasing has suddenly come on leaps and bounds recently (but it has taken a lot of practice and is still far from perfect!). Don't give up and do keep a couple of your rubbish ones-you'll be able to look back at them later on and see how much you've improved (which always cheers me up  ;D). One tip which really helped me-if you are spiral encasing twist your clear slightly backwards and forwards between your fingers as you wrap it on-it helps to push the air out and reduce bubbles.

Another thing-sometimes I think I've cocked up some encasing but I carry on heating and working as though my encasing is fine and I am surprised by how often it actually turns out ok-don't give up too early, you may be surprised  ;D
Title: Re: Encasing
Post by: garishglobes on February 09, 2008, 04:14:58 PM
Don't give up! You will get there, it just takes lots and lots of practice. Start small and work up! Just don't despair, its hard but a method that works for you will suddenly click and you'll wonder how you ever had a problem.
Title: Re: Encasing
Post by: Bumpy Beads on February 09, 2008, 05:46:52 PM
It's all been said already. One day you can't do it, next day you can!  :o

What helped me most was sitting next to another lampworker last week and actually watching her do it, and  her watching me and telling me what I was doing wrong.

Stick with it, and until you suss it take great pride in all the other things you CAN do.
Title: Re: Encasing
Post by: fionaess on February 09, 2008, 06:05:40 PM
Thanks everyone... especially Tan.. that was just what I needed.  I was cack handedly attempting to encase big beads... and actually giving myself a headache, most unusual for me..  But I took your advice Tan.. and made a little, and I mean little, pea size red bead and encased it.. and then I made a little dotty bead and encased that one... this evening I will make a little barrel and a little decorated barrel and encase both of them.  And I will leave it at that for today for my encasing. Although knowing me I will continue with the little encased beads.. I can just see them on a dangly charm bracelet  ;D  What Tan made me see was that I was trying, once again, to run before I can walk, I hate giving up on things, but now I can encase... albeit tiny beads... Thank you all  :D :D
I still find that my effetre clear very stiff... are any of the other clears better.. ie  easier to encase with?
Fiona
Title: Re: Encasing
Post by: ♥♥Tan♥♥ on February 09, 2008, 06:08:23 PM
If your down this end, come and see me and I can show you for real. Vetro is ok, not a great clear though, the better the clear teh more expensive it gets, effetre seems about the cheapest are your rods very thick?
Title: Re: Encasing
Post by: fionaess on February 09, 2008, 06:10:09 PM
Yeah... thick and non gloopy... stiff as a stiff thing, and if you heat them too hard they burn  >:(  I seem to stand for ages trying to melt the stuff. >:(

Fi
Title: Re: Encasing
Post by: Kaz on February 09, 2008, 06:14:48 PM
Quote from: fionaess on February 09, 2008, 06:10:09 PM
Yeah... thick and non gloopy... stiff as a stiff thing, and if you heat them too hard they burn  >:(  I seem to stand for ages trying to melt the stuff. >:(

Fi
!!!!!!!!!!
Kaz
Title: Re: Encasing
Post by: fionaess on February 09, 2008, 06:18:55 PM
 :D :D
Title: Re: Encasing
Post by: afina on February 09, 2008, 06:23:41 PM
There is a new kind of Lauscha clear which is really soft. And there is the new Reichenbach 104 clear, very soft, too. I like the Reichenbach very much. Don't know who carries it in the UK, though.
Title: Re: Encasing
Post by: Kaz on February 09, 2008, 06:29:42 PM
I got some of the Lauscha new clear from Q and it seems really nice - the rods are very thin to and so it melts easily and you can wrap it round several times to get the initial thickness and protect the base bead. Not cheap though :D
Kaz
Title: Re: Encasing
Post by: beadysam on February 09, 2008, 06:36:38 PM
Quote from: afina on February 09, 2008, 06:23:41 PM
There is a new kind of Lauscha clear which is really soft. And there is the new Reichenbach 104 clear, very soft, too. I like the Reichenbach very much. Don't know who carries it in the UK, though.

Interesting, I might get some 104 clear next time I stock up on Reich frit - I'll have a browse over at LE see what they think to the clear....
Title: Re: Encasing
Post by: Shirley on February 09, 2008, 06:57:14 PM
I think Martin Tuffnell has Reichenbach clear....
Title: Re: Encasing
Post by: glassworks on February 09, 2008, 07:54:51 PM
the "soft" lauscha is the new "2007" version.. not as stiff as the earlier version but juts as clear..

a certain major Italian glass maker (NOT vetrofond for a change) gave me a handful of still warm hand pulled clear rods to try - he has totally re-formulated to get rid of the reputation his clear has for being scummy and not the best quality... griet is winding beads with it as we speak (type!)...

;D ;D
Title: Re: Encasing
Post by: beadysam on February 09, 2008, 08:16:01 PM
Keep us updated Q....


Why is it the really pale transparents with just a hint of pink or blue, don't scum...? ???
Title: Re: Encasing
Post by: afina on February 09, 2008, 10:54:42 PM
Q, if Moretti would be able to make a good, non-scummy clear that has no cracking issues either, that would be just great!!! Pls keep us informed!
Title: Re: Encasing
Post by: fionaess on February 09, 2008, 11:21:23 PM
I would be really happy to test it for you Q....  ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D ;D

Fiona
Title: Re: Encasing
Post by: LesleyMac on February 10, 2008, 07:56:59 AM
Seems like Tan has been really helpful to you here because she broke it down into tiny steps and its easier to take a tiny step than climb a mountain, Tan is so clever.   ;D As for the clear, I think Laucha is brilliant however it seems to crack in bigger beads, Vetro is better than Effetre and I haven't tried any of the others. About time I did though and the Reichenback seems interesting, oh for a scum free clear, that is easy to use and doesen't crack. ;D
Title: Re: Encasing
Post by: glassworks on February 10, 2008, 10:18:20 AM
we have also just been told by gt glassworks (of black nebula and green envy fame) that they included their new crystal clear in my shipment due here tomorrow.. it is in paris now, and will be here tomorrow morning so i will check it out.. George is making all the right noises about this clear - for example he wraps each rod individually so that there are no scratches during shipment etc... we are VERY keen to see this, a even our precision104 gets a little scratched up in the shipping..

;) ;D
Title: Re: Encasing
Post by: Ilona on February 10, 2008, 10:59:25 AM
I made some larger beads for Christmas and that Launcha ones cracked.  I had never had beads cracking before. I now am usuing the Vetrofond and so far no problems. :)
Title: Re: Encasing
Post by: Bumpy Beads on February 10, 2008, 07:43:00 PM
I just remembered something else that I've found helpful. Instead of practicing encasing with clear, choose a coloured transparent over a contrasting base. That way you can see what you're doing more easily until you get the hang of it.  ;)
Title: Re: Encasing
Post by: fionaess on February 10, 2008, 10:27:34 PM
Thanks for that tip Heather.. and yes, clear is really difficult to see  :D

Fiona
Title: Re: Encasing
Post by: Ilona on February 10, 2008, 10:42:24 PM
But how do you stop the bubbles?

I like the bubbles, but not everyone does, and I think it can weaken the bead.
Title: Re: Encasing
Post by: Amber on February 11, 2008, 11:37:50 AM
I've been struggling with encasing too, but I love the effect, so WILL NOT let it beat me! I keep thinking I've mastered it, but then find that a tiny bit of the core has 'escaped'...same thing every time!  :( It does seem like part of the problem is that the clear is so stiff that by the time you've melted it the core is melting too.

Good tips though - I'll try Tan's tip and some different transparents and see what happens!
Title: Re: Encasing
Post by: littlegiggles on February 11, 2008, 12:18:41 PM
I've tried encasing on and off since i started in july 06... and suddenly mastered it on little beads... just came over night... I had no probs with murrini but I just couldnt make encased round beads.. so it really is that PPP
Title: Re: Encasing
Post by: Hil on February 11, 2008, 12:55:47 PM
I have been practising on and off using coloured transparents instead of clear, as I only have effetre clear and it is a sod!  I have found that using BeadySam's PushyPully tools are a great help as you can push the glass right up to the mandrel (being careful not to let it touch the mandrel).  I also just add the odd dots of extra glass wherever it is needed so as not to make the bead too large.

Hil x
Title: Re: Encasing
Post by: Amber on February 13, 2008, 05:00:44 PM
Tan, you're a hero!  :D

I tried out Tan's tip and made a tiny core bead - just one skinny wrap of glass - then I pretended to myself that I wasn't trying to encase and wrapped the transparent over the top, as I would a normal bead onto the mandrel. And here's the result!

(http://i171.photobucket.com/albums/u286/Spookyjewel/Encased.jpg)

I'm soooo chuffed. Not perfect yet, but definitely getting there!  8)
Title: Re: Encasing
Post by: Sal on February 13, 2008, 05:05:51 PM
They're really pretty  ;D Must give it a go myself
Title: Re: Encasing
Post by: fionaess on February 13, 2008, 05:09:50 PM
Yesssss Amber  ;D ;D ;D ;D ;D

Fiona
Title: Re: Encasing
Post by: Amber on February 13, 2008, 05:52:31 PM
Sorry for hijacking your thread Fiona, just couldn't contain my excitement!
Title: Re: Encasing
Post by: fionaess on February 13, 2008, 07:09:03 PM
Hey Amber.. its not my thread... its our thread  ;D ;D ;D

Fiona
Title: Re: Encasing
Post by: Kaz on February 13, 2008, 09:09:52 PM
Those look great Amber.
Kaz
Title: Re: Encasing
Post by: glassworks on February 14, 2008, 10:32:50 AM
well done, both to amber and to tan!..  ;D
Title: Re: Encasing
Post by: fionaess on February 16, 2008, 07:50:15 PM
Emma very kindly sent me some nubs of rods... odds and ends.. and some of them were clear.. so I pulled them into stringers and used them about 20 mins ago to see if I could encase..... oh frabulous bliss...whatever glass it is melts beautifully, doesn't burn, I'm in heaven.. but I don't know what glass it is.  I've pm'd Emma to ask her, and when I find out I will post a pic of my first encased bead, and the glass as well..
I am so verrrrrrry pleased, I honestly thought it was my sheer incompetence and impatience, mind you 30 mins to encase a bead is a bit too long :D  The one and only, which I have just done, took around  5 mins... Im a Happy Bunny  :D :D :D :D

Fiona
Title: Re: Encasing
Post by: Amber on February 16, 2008, 09:18:19 PM
Pics!  :D

It's a great feeling, isn't it?!
Title: Re: Encasing
Post by: fionaess on February 16, 2008, 10:51:29 PM
Pics... well which half of the beautiful bead do you want to see.... I took it out of its blanket and found it in two pieces.. thermal shock had set in .. probably because I had actually managed to make an encased bead  :D
But I'm off to make another one, if I can do it once, I can do it again, with my nub stringers  ;D ;D

Fiona
Title: Re: Encasing
Post by: June on February 16, 2008, 11:10:00 PM
Oh no, Fiona !  Why does that happen?  ::)  Still, as you say, if you can do it once, then maybe you have already created another - so better luck with this one !   ;D
Title: Re: Encasing
Post by: flowerjasper on March 02, 2008, 06:03:54 PM
i have just been to the essex bead fair,
i picked up my order from martin (tuffnells glass) i also treated myself to some CIM glass,
cim cerris is a cloudy clear, pearly,
thought i would try it over some trans blue.... low and behold the best clear encased bead i have done!!
melted really easily,
sandy
Title: Re: Encasing
Post by: Shirley on March 02, 2008, 06:25:23 PM
Nice one! Just stick with it. It gets easier to 'read' the glass as you get more experienced.