How do I make an encased stringer please ???
Fiona
You heat the clear/ transparent rod to very melty and swipe it down the other rod (warmed first) then keep it barely warm while melting another load to swipe down other side, then warm whole thing and pinch together the gaps with tweezers. then warm and pull like a stringer.. Clear? As mud I expect, I should leave it to the experts, but I have just done some of these today ;D