Frit-Happens !

Tutorials in here.. => Glass fusing => Topic started by: ♥♥Tan♥♥ on January 25, 2008, 08:58:01 AM

Title: E6000 tut
Post by: ♥♥Tan♥♥ on January 25, 2008, 08:58:01 AM
http://www.ugotglass.com/E6000.htm
Title: Re: E6000 tut
Post by: julieHB on January 25, 2008, 09:18:13 AM
Thanks, Tan!  I have got myself a tube of E6000, but not tried it yet.  Good to get some pointers  :D

Julie
Title: Re: E6000 tut
Post by: GoodMonkey on January 25, 2008, 09:53:36 AM
Thats brilliant, the way it's written made me smile as well - thanks Tan
Title: Re: E6000 tut
Post by: ♥♥Tan♥♥ on January 25, 2008, 10:06:12 AM
Me and E6ooo and a 'thing', it's not a good thing, in fact, it gets quite violent at times, but maybe,,,,,,just maybe these tips may help salve our troubled waters
Title: Re: E6000 tut
Post by: Zeldazog on January 25, 2008, 04:19:16 PM
Tan

I got all excited then that you'd found some new advice regarding E6000 - unfortunately, I have already seen that one and followed its instructions... perhaps its just me.......

Don't let that put anyone off though - I think all the glues in the world have a conspiracy against me!


Title: Re: E6000 tut
Post by: DragonflyLynne on January 25, 2008, 05:50:04 PM
Thanks Tan  ;D
Title: Re: E6000 tut
Post by: ♥♥Tan♥♥ on January 25, 2008, 06:30:28 PM
Dawn, I suspect it may be the two of us ;)