Title: Clean lentil ends?
Post by: sparrow on January 09, 2008, 08:26:13 AM
Mine are very hit and miss, and I'd like to avoid the burrs  ;D - any good tips?
Title: Re: Clean lentil ends?
Post by: Redhotsal on January 09, 2008, 09:10:19 AM
If you are having  burrs it sounds like your "footprint" is too long - i.e. the glass is spread too far along the mandrel before you apply the press. Try shortening the length of the footprint.
Title: Re: Clean lentil ends?
Post by: GoodMonkey on January 09, 2008, 09:32:41 AM
Hiya Sal
Title: Re: Clean lentil ends?
Post by: GoodMonkey on January 09, 2008, 09:33:30 AM
Sorry Sabine I can't help you I've not got a lentil press - would like one though.
Title: Re: Clean lentil ends?
Post by: Redhotsal on January 09, 2008, 09:37:31 AM
HI Shelley  :D
Title: Re: Clean lentil ends?
Post by: beads-on-toast on January 09, 2008, 09:46:30 AM
yep

Sal is correct

the straight sided presses require you to go right up to the edge, however, due to the nature of the lentil shape i always leave it a few mm or so short at the ends
Title: Re: Clean lentil ends?
Post by: sparrow on January 09, 2008, 09:57:37 AM
Thanks, that makes sense now - I started with a spree and applied the same principle  :D You guys rock! Will make lentils later today!
Title: Re: Clean lentil ends?
Post by: turnedlight on January 09, 2008, 11:40:02 AM
And if you need more glass, try not to add right at the ends :)
Title: Re: Clean lentil ends?
Post by: *rowanberry* on January 09, 2008, 12:57:37 PM
I find pressing them from a round bead, and pressing while quite cool (ie you have to use a fair whack of pressure!) works very well for me. I used to do rugby ball shape, but weirdly found i got a better shape from something rounder.

I can show you next friday if thee wants?
Title: Re: Clean lentil ends?
Post by: sparrow on January 09, 2008, 01:31:56 PM
Quote from: *rowanberry* on January 09, 2008, 12:57:37 PM

I can show you next friday if thee wants?

Oooh, the list of what you're showing me grows :) :) Thanks! I'll give it a go next time Toby lets me, then I'll finetune next Friday :)

By the way, are you partial to any particular form of cake or chocolate?
Title: Re: Clean lentil ends?
Post by: *rowanberry* on January 09, 2008, 02:00:04 PM
I'm dietting at the moment - so very keen on Weight Watchers Eclairs :D which are DIVINE!
Maybe you can send me a list of what you'd like to learn in advance? so I make sure I know it, lol!
Title: Re: Clean lentil ends?
Post by: mariag on January 09, 2008, 05:28:20 PM
Ooooh I wish I lived near you lot.....a glassy get together & WW eclairs - yum yum!! ;D
Title: Re: Clean lentil ends?
Post by: Vicki on January 09, 2008, 05:48:59 PM
if they are wight watchers, does that mean you can eat more ;D  oh stop me, I'm trying to lose a bit myself...I did realy well until I have 8 cubes of choccie that was the last of my xmas bar....I guess it gone now & will stop shouting at me from the fridge ;D
Title: Re: Clean lentil ends?
Post by: *rowanberry* on January 09, 2008, 06:33:16 PM
1.5 points per eclair if i remember :D hmmmmmmmmmm
and yes it means you can scoff 3 in a go and not feel totally guilty!
Title: Re: Clean lentil ends?
Post by: Vicki on January 09, 2008, 07:00:07 PM
 :P....tomorrow I'm going to be realy good, I've started running again, but I can feel all the extra weight I've gained during my 10 & a bit months of lampworking dragging in the pavement ;D
Title: Re: Clean lentil ends?
Post by: sparrow on January 10, 2008, 09:11:31 AM
Thank you very much, everybody, I can dutifully report that my lentils are now smooth-ended  ;D Made my day yesterday!!  ;D ;D
Title: Re: Clean lentil ends?
Post by: Kaz on January 10, 2008, 11:42:58 AM
Photos, photos, photos.......please :-*
Kaz
Title: Re: Clean lentil ends?
Post by: *rowanberry* on January 10, 2008, 11:55:00 AM
yay! way to go Sabine!