Frit-Happens !

Lampwork => Borosilicate => Topic started by: Marcel on December 22, 2015, 03:21:45 PM

Title: some new work
Post by: Marcel on December 22, 2015, 03:21:45 PM
Here is some of my latest work :)

(http://s28.postimg.org/omhdhhizd/IMG_0173.jpg) (http://postimg.org/image/omhdhhizd/)

(http://s28.postimg.org/4t59os5ll/IMG_0178.jpg) (http://postimg.org/image/4t59os5ll/)

(http://s12.postimg.org/s92pu2py1/IMG_0193.jpg) (http://postimg.org/image/s92pu2py1/)

(http://s12.postimg.org/9oehn04ih/IMG_0194.jpg) (http://postimg.org/image/9oehn04ih/)

(http://s12.postimg.org/mwdvfy21l/IMG_0195.jpg) (http://postimg.org/image/mwdvfy21l/)

(http://s12.postimg.org/6k3tq7nq1/IMG_0196.jpg) (http://postimg.org/image/6k3tq7nq1/)

(http://s13.postimg.org/5l4of8oir/PICT1048.jpg) (http://postimg.org/image/5l4of8oir/)

(http://s13.postimg.org/j0rp4ox0j/PICT1054.jpg) (http://postimg.org/image/j0rp4ox0j/)
Title: Re: some new work
Post by: Rascal on December 22, 2015, 03:29:11 PM
Stunning work as always, my favourites are the hearts.
Title: Re: some new work
Post by: Marcel on December 22, 2015, 03:35:32 PM
Thank you ;) there fun to make too :)
Title: Re: some new work
Post by: Margram on December 22, 2015, 06:25:10 PM
Great work! I love the ruffled effect in the last one - like waves  :)
Title: Re: some new work
Post by: Moira HFG on December 22, 2015, 07:15:10 PM
All wonderful! I especially like the tooth. And the ruffly waves.
Your work is always beautiful  :)
Title: Re: some new work
Post by: mel on December 22, 2015, 09:39:07 PM
Really good, to me the texture looks like it could be ancient tool marks on napped flint arrows or axe heads. Does it feel smooth or is there surface texture? It's difficult to tell.
Title: Re: some new work
Post by: GaysieMay on December 23, 2015, 05:27:26 PM
Love your new work Marcel. X
Title: Re: some new work
Post by: ajda on December 24, 2015, 07:38:50 AM
Quote from: Rascal on December 22, 2015, 03:29:11 PM
Stunning work as always, my favourites are the hearts.
You took the words out of my mouth - though my favourites are the "prehistoric" pieces, especially the toothy one.

Quote from: mel on December 22, 2015, 09:39:07 PM
Really good, to me the texture looks like it could be ancient tool marks on napped flint arrows or axe heads. Does it feel smooth or is there surface texture? It's difficult to tell.
Looks to me as if some of the textures are impressed on the hot glass (the 2 leaf-shaped ones), but that he's cold-worked the two hearts at the bottom, grinding the texture so it looks carved or napped - a technique we've seen Marcel use before to great effect. But I shouldn't be trying to speak for him... Marcel, step forward and explain yourself!

There's a guy on Murano, Luigi Camozzo, who does cold-working that reminds me of Marcel's - see https://www.youtube.com/watch?v=dsD0DvJMsQ0 and fast forward to around 20 mins into the video.
Title: Re: some new work
Post by: Marcel on December 24, 2015, 09:49:13 AM
Thank you all and your right i dremeled the heart for a rough texture :)
it is hollow blown by the way :)
i am glad you guys like my work :)
Title: Re: some new work
Post by: Marcel on December 24, 2015, 09:52:16 AM
great video of  Luigi Camozzo!! thank you for sharing :)
Title: Re: some new work
Post by: Moira HFG on December 24, 2015, 11:41:19 AM
I love that carving technique and the texture it produces. Great video; and thanks for the reminder Marcel, all you need is a Dremel for small work. Another thing on the 'must try that' list.

I loved these pieces which I saw in Murano last June (and I'm happy to be remined of June, in this weather!):
http://www.inexhibit.com/marker/venice-the-sculpture-of-vistosi-at-the-murano-glass-museum/
They are blown, then finely carved over the whole surface.
Title: Re: some new work
Post by: baked glass on February 03, 2016, 09:00:29 AM
very nice, I'm impressed with the hollow heart.  I've been trying to do some blown shapes and it's difficult to get good symmetry.  :)
Title: Re: some new work
Post by: tuffnell glass on February 03, 2016, 09:28:06 AM
Hi Marcel,
                  Love your work and can't wait to see it in June.

Best wishes,

Martin
Tuffnell Glass
Title: Re: some new work
Post by: flame n fuse on February 03, 2016, 05:12:48 PM
it's all beautiful, and such a range of styles
Title: Re: some new work
Post by: Marcel on February 08, 2016, 07:53:02 PM
Thank you my friends :)
Can't wait to visit you Martin :) and thank you for the compliments
Title: Re: some new work
Post by: Marcel on February 12, 2016, 08:36:52 AM
Thank you for responding  :) i always love to read the comments.
and am glad you all like my work.