Hi,
We have just received a delivery from Northstar which included a small amount of ill-uminati (we ordered loads but all distributors are on limited orders).
As well as ill-uminati we have added another 5 new colours which are Mystery Aventurine, Bubblegum, Silver Unobtainium, Irrid and Sublime
(http://tuffnellglass.com/contents/media/t_ns-62-bubblegum.jpg) (http://tuffnellglass.com/contents/media/t_ns-14-irrid.jpg) (http://tuffnellglass.com/contents/media/t_ns-120.jpg) (http://tuffnellglass.com/contents/media/t_ns-78-mystery-aventurine.jpg) (http://tuffnellglass.com/contents/media/t_ns-66-sublime.jpg)
These and more are all on ,
http://tuffnellglass.com/contents/en-uk/d316_Northstar_Coloured_Borosilicate_.html (http://tuffnellglass.com/contents/en-uk/d316_Northstar_Coloured_Borosilicate_.html)
Best wishes,
Martin