Lampwork => COE 104 => Topic started by: Fluffstar on June 12, 2015, 08:16:58 PM

Title: Reichenbach CoE
Post by: Fluffstar on June 12, 2015, 08:16:58 PM
Hi All,

Sorry if this has been asked already - I did a search but nothing concrete.

Does Reichenbach make rods with 2 different CoE's?  Only there are Reichenbach rods for sale at Tuffnell's advertised as 104, and on beadbug it's 94 +/- 2...

Sorry if it's a dumb question.  Thanks!

Kathy.
Title: Re: Reichenbach CoE
Post by: flame n fuse on June 12, 2015, 08:37:41 PM
yes, there are 2 types