Hi
Has anyone used this much .. is it a stiff white. I'm looking for an alternative to CiM ... effetre is too soft!
TIA
I use Reichenbach white but I can't honestly say that I've noticed whether it's any stiffer than effetre. I switched from effetre when Martin ran out one time and I hated using effetre soft white. That's like frit on a stick. It does improve if you anneal it before using but who want to be aXXed with that.
Lol Pat ... you are funny
I haven't used Reichenbach White, but I tend to find their other colours stiffer. Btw, I picked my glass swap up from post office the other day - thank you, lots of yummy glass to play with!
hee hee ... enjoy x