I just wondered if anyone had much experience in fusing with spectrum 96.
It seems to be slightly cheaper than bullseye and is softer so in theory easier to cut apparently.
Also, would any one know of any UK suppliers of per cut spectrum clear circles.
Thanks,
Sarah x
I've done some fusing with Spectrum 96 as I had a lot left over from making stained glass windows. You might try http://www.leadandlight.co.uk/ but if you can already cut circles with Bullseye, Spectrum would be no problem. Look at https://www.youtube.com/watch?v=1mmnslCq5UM for one video on cutting circles freehand or just search on youtube for "how to cut glass circles". The Spectrum waterglasses (transparents) are especially good and make great beads too when cut into 1/4 inch strips.