Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Ventilation => Topic started by: Sam on December 23, 2007, 12:23:32 PM

Title: ventilation
Post by: Sam on December 23, 2007, 12:23:32 PM
Hi,

I've been lampworking in the conservatory without any proper ventilation system just open windows :-[


Have you guys got any ideas how I should go about setting up a ventilation system bearing in mind that I don't have a wall I can attach anything to as the conservatory is off our dining room! :-\

Also, where do you get these things ???

Any help would be gratefullu appreciated!!!



Sam ;D

Title: Re: ventilation
Post by: Shirley on December 23, 2007, 01:23:02 PM
I've got a hydrophonics extraction fan that seems to do the trick. I got a flexible hose so it can be vented outside, in my case through the garage door, but it could be through a window. Got it from Ebay - the guy put a normal plug on it rather then it having to be wired in. Ebay seller was spares_4_all but he doesn't seem to have any listed at the moment. Might be worth contacting him.
Title: Re: ventilation
Post by: Mary on December 23, 2007, 04:38:49 PM
I'm in the conservatory too, so to get round the "no wall" problem, hubby built me a freestanding box round the table. The fan is in the "ceiling" and it vents out a window. Here's a pic of it half done.

(http://i123.photobucket.com/albums/o297/weemaryanne/Mylampwork140.jpg)
Title: Re: ventilation
Post by: Sam on December 28, 2007, 10:07:14 AM
Thanks Shirley and Mary,


Mary, do you have a pic of what's in the ceiling?

I have told DH all about what your hubby has done and that he's got to sort something out TODAY!!

No more Scrap heap challenge, Top Gear and Places in the sun until he comes up with a few ideas!

Guess what he works in ??? Yes that's right VENTILATION!!!

He says he doesn't know a thing about oxyconx though!!

Any ides what I should do with him guys ??? ??? forget the ventilation!


Sam. ;D
Title: Re: ventilation
Post by: Sandra J on December 28, 2007, 10:41:44 AM
QuoteAny ides what I should do with him guys forget the ventilation!


Sounds like a good idea! Don't know how long he'd last without oxygen though!  ;D
Title: Re: ventilation
Post by: Sam on December 28, 2007, 11:54:05 AM

He can survive on beer, no worries there!


I'd consider trading him for some vetrofond, any offers ???



Sam.
Title: Re: ventilation
Post by: Mary on December 28, 2007, 12:25:43 PM
Well Sam, now my desk is facing the window. The small fanlight window is removed and the ducting fitted straight to the opening. So the fan (mine is a big Expelair he got through his work, but a cooker hood would do) is in the box ceiling, with ducting running from it.

The box also has sides and a front lip. Enclosing it a bit helps make it more efficient. It also has spotlights mounted in it, lol!
Title: Re: ventilation
Post by: mariag on December 28, 2007, 03:52:50 PM
I've got a cooker hood set up in my shed, we got it from Wickes for £40.
Title: Re: ventilation
Post by: Sam on December 28, 2007, 04:35:07 PM
Thankyou ALL very much for all your help.


He's agreed to go to Wickes tomorrow!! ;D

Watch this space!!!!!!!! ;)



Sam.
Title: Re: ventilation
Post by: Sam on December 30, 2007, 10:15:47 AM

Got him to Wickes & B&Q yesterday yay ;D

DH bought some white coil like tubes and small square boxes!

Still in the bags but it's progress ;D Nagging really does work!!

Will keep you posted!



Sam
Title: Re: ventilation
Post by: LittleMoo on December 31, 2007, 08:48:55 PM
Half way there Sam! I bought an extractor cooker hood from Ikea for £35 back in Aug and DH has just got round to fitting it today - woohoo!!! No more torching in the cold shed with the door wide open!  ;D
Title: Re: ventilation
Post by: Sam on December 31, 2007, 09:33:33 PM

Great News Littlemoo! ;D



Sam.