Hi

I was just wondering if anyone has used the warm glass printable decals with a Dell laser printer?

The listing says HP and Canon, but we've got a Dell.

TIA
Title: Re: Warm glass printable decals - work with a dell printer?
Post by: Zeldazog on November 10, 2014, 05:38:27 PM
It needs iron content in the printing product to work, so if you can find a materials spec for the toner cartridge, does that give any info?
Title: Re: Warm glass printable decals - work with a dell printer?
Post by: RLBrown on November 10, 2014, 10:22:36 PM
Ah. Now I know what to look for... Thanks


I've just googled the MSDS for my printer and it appears not :-(

Oh well still other options. And lots of other techniques to try.