Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: Chef7272 on November 01, 2014, 04:01:35 PM

Title: Glassline Pens
Post by: Chef7272 on November 01, 2014, 04:01:35 PM
Hi All,

Just a quick question about Glassline pens.  I was wondering what these should look like after firing?  I have just bought some and used them for the first time.  I was expecting them to come out with a gloss finish but they are coming out matt.  I have only taken them to a tack fuse temperature so far.  Would taking them to full fuse temperature make them glossy? or do I need to look as using enamels for a gloss look?

I have to say the effect I have got with the Glassline pens is really great and is one of these happy accidents which will be used in other ways.  Just not what I had intended  ;D

Thanks all in advance

Peter