Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: RLBrown on October 26, 2014, 09:22:56 AM

Title: Angel face?
Post by: RLBrown on October 26, 2014, 09:22:56 AM
Hi

My daughter has asked me to make her a glass angel but I'm not sure what colour to use for the face.

I'm a bullseye girl so was thinking of light peach cream (0034). Is this a good choice?
Title: Re: Angel face?
Post by: Rachels on October 26, 2014, 12:38:28 PM
Hi, Yes that's the colour I use for all my faces when I am fusing.  Rachels.
Title: Re: Angel face?
Post by: RLBrown on November 10, 2014, 04:15:16 PM
Thanks for the advice.

I ordered some of the light cream... Just waiting for my kiln to be plugged in.