Title: EASY GLASS SILHOUETTE TUTORIAL
Post by: DeePoole on September 20, 2014, 06:49:05 AM
This is really effective! Not to mention easy....I hope you enjoy it, Dee x
http://www.youtube.com/watch?v=NQ-kiIaJ-cA (http://www.youtube.com/watch?v=NQ-kiIaJ-cA)
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: marklaird on September 20, 2014, 08:52:54 AM
Hi Dee. That's really effective. Thankyou for sharing.
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: Glyn Burton on September 20, 2014, 09:44:54 AM
Why not just draw it on with grisaille
Title: Reply to Glyn
Post by: DeePoole on September 21, 2014, 05:01:59 PM
Hi Glyn,
Why don't I use grisaille? 'cos I like this way best. It's all a matter of preference in the end, there are many ways to achieve an effect aren't there? There's something out there for all of us.
I've made silhouettes using stencils and powder and fuseable paint and I love this method best of all. xx
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: Glyn Burton on September 22, 2014, 08:18:16 AM
Didn't mean to cause offence I was just curious.
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: DeePoole on September 22, 2014, 09:32:59 AM
No offence taken Glyn... my home made videos are only a starting point for fusers that's all. I don't think experienced fusers would watch them very much.
I've had some good sales from personalised glass silhouettes, so others might do too.

Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: shafeenan on January 17, 2015, 09:55:29 AM
Um - what's grisaille? sounds interesting.....BTW  Can't tell you how helpful Dee is - a mine of info, brill tutorials for newbies!
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: Pat from Canvey on January 17, 2015, 02:46:43 PM
Have a look at http://en.wikipedia.org/wiki/Grisaille
Title: Re: EASY GLASS SILHOUETTE TUTORIAL
Post by: shafeenan on January 18, 2015, 11:58:20 AM
Thanks Pat - looks way beyond me at the moment...indeed possibly forever!