Frit-Happens !

Lampwork => COE 104 => Topic started by: shelly on July 07, 2014, 06:32:39 PM

Title: stringers
Post by: shelly on July 07, 2014, 06:32:39 PM
Ok, I have been following tutorials on stringers and still am doing something wrong as they dont seem to soften in the outside bit of flame as explained in one tutorial so i move in and end up in the flame and them dissolving into dots.

Any advice on what i am doing wrong or is it a case of just keep trying as am getting very frustrated with it.
Title: Re: stringers
Post by: lampworklover on July 07, 2014, 08:03:46 PM
Pretty much halfway between the two! Start a long way out, then very gradually move the stringer in until the end is just soft. Try and move the bead, not the stringer. Pretty much one of the harder things to master IMHO, but you will get there with 'PPP'.
Title: Re: stringers
Post by: shelly on July 08, 2014, 09:45:43 AM
Thankyou, will keep trying then, would like to be able to do it.
Title: Re: stringers
Post by: flame n fuse on July 08, 2014, 10:03:22 AM
yes, it's really hard. I can make curls in one direction, but not the other!. I have tried several tutorials but they haven't helped me. Can anyone tell me which tutorial really gave them the break through?
Title: Re: stringers
Post by: lampworklover on July 08, 2014, 10:10:58 AM
Don't think I have ever used a tutorial, but then I'm not one for written instructions (visual learner).
Title: Re: stringers
Post by: DementedMagpie on July 08, 2014, 01:44:40 PM
There's a Laura Sparling video (http://www.youtube.com/watch?v=Eei0n8z_1uc) which I find quite helpful.

Otherwise, it's a matter of practice. And one day I will have done enough of it, and my stringer work will be good enough...
Title: Re: stringers
Post by: lampworklover on July 08, 2014, 01:53:01 PM
Quote from: DementedMagpie on July 08, 2014, 01:44:40 PM

Otherwise, it's a matter of practice. And one day I will have done enough of it, and my stringer work will be good enough...

LOL, you and me both! :D
Title: Re: stringers
Post by: ARBeads on July 08, 2014, 03:26:53 PM
Really is a practice thing with additional sacrifices to the Kiln fairies!

Start with a cheap transparent, they're a bit stiffer. Make a base bead of the same transparent and then start practising, each time you go wrong melt in the stringer work and start again.

On some torches you can turn down the flame to a pinpoint others it's all about finding the 'sweet point' which is of to one side. You may find a combination of both works for you.

For straight stringer application (across or around bead) I work directly underneath the flame, bringing both the stringer and the bead up toward the bottom of the flame till the stringer bends around the bead circumference, the stringer should not be glowing.

My problem is I'm inconsistency, one day I can do a full set of Scroll beads the next all I can do is dots!

Title: Re: stringers
Post by: flame n fuse on July 08, 2014, 04:18:25 PM
with straight fine stringer, I find that warming the bead and laying the stringer on the hot bead works quite well, but can't do accuracy, or reliable scrolls.
Title: Re: stringers
Post by: DementedMagpie on July 08, 2014, 04:34:43 PM
I remember the JC Herrell demo at Flame Off: I reckon about half the audience, me included, was thinking something along the lines of "How does she do that? Is that magic?"
Title: Re: stringers
Post by: flame n fuse on July 08, 2014, 06:07:49 PM
I think she says that you need to do 2000 beads before you get one that's perfect
Title: Re: stringers
Post by: lampworklover on July 08, 2014, 08:48:48 PM
Quote from: flame n fuse on July 08, 2014, 06:07:49 PM
I think she says that you need to do 2000 beads before you get one that's perfect

way past that and mine are still rubbish  ;D