Frit-Happens !

Challenges, Competitions, Swaps & Loans => Monthly Challenge => Topic started by: beads-on-toast on December 07, 2007, 10:27:34 AM

Title: COLOUR 10- SILVER - DEC07-Jan08
Post by: beads-on-toast on December 07, 2007, 10:27:34 AM
Here it is!

This is the tenth colour challenge on Frit happens and it is for two months as i know how busy we all are over the xmas period, and it is

SILVER

This is inspired by the FOIL/LEAF thread that has been started and also the lack of Silvered glass i use!!!

You can make anythin that takes your fancy however it must contain silvered glass (Double Helix) Maybe Silver Plum, Foils, Leaf the possibilities are ENDLESS!!!

A focal, a set a critter it is completely up to you.


Sound good?

So lets go!!!

The next Colour challenge will be started in February
Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: Clare Scott on January 10, 2008, 06:39:56 PM
Some DH from me....

Aion and Psyche (over reduced)

(http://i168.photobucket.com/albums/u197/northernsockmonkeys/363.jpg)

Nyx with Silver Leaf

(http://i168.photobucket.com/albums/u197/northernsockmonkeys/362.jpg)

My good ol' planets! Psyche.

(http://i168.photobucket.com/albums/u197/northernsockmonkeys/209.jpg)

Aion Nuggets

(http://i168.photobucket.com/albums/u197/northernsockmonkeys/344.jpg)

Gaia Bicone

(http://i168.photobucket.com/albums/u197/northernsockmonkeys/364.jpg)

Sorry for the hog...I would sell my soul for this glass. :D

Clare xx
Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: afina on January 10, 2008, 10:48:31 PM
Hi!
Just wanted to show you a crunched bead I made with Ornela ivory covered in silverleaf, then burnt the silver in, did some scrollwork with a transparent stringer and then reduced the bead (after pressing and firepolishing).
(http://www.glasperlenwerk.at/images/stories/Einzelperlen/goldcrunch.jpg)

It looks as if it were covered in goldleaf, but it was silverleaf.
Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: sparrow on January 11, 2008, 05:25:29 PM
They are lovely, everybody. I love that Nyx & silver leaf set. Verena, that bead is gorgeous!

Thought I'd play this month - anything clear and sea-like I had flying around, silver foil, and some of beadysam's fun'n'funky frits:

(http://farm3.static.flickr.com/2238/2185069487_c5d10e9642.jpg)
Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: LesleyMac on January 16, 2008, 09:36:24 AM
Absolutely stunning silver beads on here, my turn then, its hard to choose as most of mine have silver in them somewhere.

I call this one silver tipped

(http://www.lesleymcfarland.com/Beadies25/Silver%20tip%20bead.jpg)

This is a set of kronos beads

(http://www.lesleymcfarland.com/Beadies25/Bead%20set2.jpg)

and this is silvered and enamelled


(http://www.lesleymcfarland.com/Beadies25/Silver%20enamel2.jpg)

Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: sparrow on January 22, 2008, 04:51:50 PM
Some more from me:

(http://farm3.static.flickr.com/2091/2211094471_b7a8f4be83.jpg)

And then.......I always wondered how people get to a signature bead, develop their own style.....there is so much to play with....but I love doing these:

(http://farm3.static.flickr.com/2297/2211094167_33657591e7_o.jpg)

(http://farm3.static.flickr.com/2320/2212466366_fb6d41f60e.jpg)

:) :)
Title: Re: COLOUR 10- SILVER - DEC07-Jan08
Post by: Sarah on January 22, 2008, 11:40:31 PM
Great beads everyone  :)

Sabine - that middle frosted one is beautiful!

I've been playing with the Barley Bead recipe in PTF

(http://farm3.static.flickr.com/2388/2212518231_0dc075de88_m.jpg)

(http://farm3.static.flickr.com/2236/2212518219_07702fb1e0_m.jpg)