Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: sandmor1 on April 15, 2014, 10:45:36 AM

Title: 2 layer insert
Post by: sandmor1 on April 15, 2014, 10:45:36 AM
I am hoping for some help with this...

I made a tile 25cm x 125cm with scraps and a clear layer. It turned out very nice but a bit ITT for a single piece. I would like to slice it into maybe 3 strips and incorporate the  strips into 3 new pieces. The first one I have in mind is to place the strip in the middle of 2 outside pieces with a clear layer on the bottom but as the middle section will then be 3 layers and the outside sections only 2, I'm not sue if this is acceptable.

Could someone advise me on this please.

Thank you

Sandra
Title: Re: 2 layer insert
Post by: Nicknack on April 15, 2014, 12:16:31 PM
You could always put a layer of clear over the outer layers, that would even it up.

Nick
Title: Re: 2 layer insert
Post by: sandmor1 on April 15, 2014, 01:08:04 PM
Thanks for that, Nick. I will put on the extra layer of clear on either side.

Sandra

Title: Re: 2 layer insert
Post by: sandmor1 on April 16, 2014, 08:55:27 AM
Hi Nick, I just want to let you know that the tile has come out perfect. I am delighted with it. It is now back in the kiln on the slump mould.

It is very heavy, well it would be, being 3 layers thick.

I suppose I should have thought myself of adding an extra layer to the sides but I am a novice...that's my excuse anyway. ;D

Thanks for taking the time to reply, I appreciate the help.

Sandra
Title: Re: 2 layer insert
Post by: Nicknack on April 16, 2014, 09:45:07 AM
You're very welcome!  I'm glad it worked well. :D :D

Nick x