Hi,
Does anyone know what Jo Downs uses for her silver inclusions. It can't be silver foil as they are sold too cheaply.
Thanks Penny
Could be mica. Janet
Thanks but it's more like its a sheet like copper foil but they sell them too cheaply for it to be silver foil. I did e mail and ask but no response! Surprise!
maybe a secret ingredient she likes to keep to herself which is fair enough ;)
Sorry, should have been more specific, mica mixed with flexi-glass made into sheet and cut up can look like silver or gold foil. I don't know what Jo uses, but this is an alternative to foils. Janet
Wow! Thank Janet. I didn't know that. Are there any instructions on how to do that anywhere?
http://www.fxnglass.com/fxnglass/Flexi-Glass.html This is there web site, there are also videos on you tube.
You can buy the stuff from warm glass, but i think they are out of stock at the moment. Janet
Thanks again. Will look.