I have recently bought the Photo Fusing Decal Paper and booklet from Warm Glass and, like Gaynor in a thread from 2012, I also was very disappointed at paying so much for the booklet which is little more than a pamphlet. At the moment, with the special offer on the paper, the booklet costs a massive extra £26!
Anyway, that's not the point of this post :)
Has anyone else used decals that they have printed themselves on fused glass rather than beads? I went mad and bought a laser printer and have had some success with trying out different fusing schedules, but would like to know if there are any tips for editing/printing B&W photographs and the type/colour of glass to use as a backing. Warm Glass has several different white opal glasses for example; are some better than others for this application? My main interest is in using landscape photographs of the Lake District, but I am trying a few other things as well.
So far, all my attempts have been with the decal on top of two layers of glass, but has anyone tried capping a decal - presumably after tack firing to the bottom layer first. Will it lose less colour if capped than it does at a full fuse when on top?
As you can tell, I have loads of questions!
Hi,
I won't be able to answer your questions as to printing your own decals and then fusing but think you may be interested in the following:
I looked at this paper yonks ago the same as you have bought, and thought it was very limited by only giving a serpia tone; I also looked at there printing offer but, for the cost of serpia it was a no.
I am getting all of my work reproduced in full colour by these guys: http://digitalceramics.com/shop/Digital%20Ceramic%20Transfer
They print full colour on a SRA3 and is an extra 15% larger print area than regular A3 size.
I would suggest you have a go with the paper you have, and let us know.
Cheers,
Lou
x
Lou, are these ceramic decals for kiln firing onto glass? There is no mention of it.
Quote from: Angie on February 22, 2014, 08:35:10 PM
Lou, are these ceramic decals for kiln firing onto glass? There is no mention of it.
Yep they are ;) Just the same as any other decals, but fire lower. I have tried a few with very good results, though only fired on top and not in between.
Bailey Decals will also run one off prints - though have not asked for a price yet - same heat/method process
When I have made decals I used the screen printing method, printing with enamel onto gummed paper and then putting a layer of cover coat on top. This is a liquid plastic which dries to make the top layer of the transfer a bit like cling film with the image stuck to it, when it burns off the fumes are not very pleasant so I should imagine if it is trapped between layers of glass it would cause problems.
Bear in mind that I was making decals for ceramics some years ago so there may be some new super duper materials on the market now which dont have the save drawbacks but I am just too old to know about.
Thank you Lou, I had a look at the page you suggested, but will experiment with what I have first. I am learning a lot from this!
Do you know the book Glass and Print by Kevin Petrie ? it may be worth a look, you can get it from Amazon uk.
No, I've not heard of that and will check it out. Thank you Glyn.
I'll chip in my twopence worth too.....if you are working with flat glass, have you thought about screen-printing directly onto the glass instead of decals? That way you could use a variety of colours in both enamels and base glass rather than being restricted to white.
It also means you don't need to use oil based mediums for making decals that can be quite nasty burning off in the kiln.
(I use and sell on a range of ready mixed enamels too, if you wanted any information about them.)
Hi Rachel,
I have no idea about how to make a screen or whether it would be viable in the space available here (my kitchen), or whether it's possible to get the detail needed for the landscape photos that I want to fuse, using the size of glass sheet that will fit into my SC2 kiln. Any online references to making screens would be welcome :)
At Art in Action the other year I bought a set of your ready mixed enamels but had problems with getting the firing temp. correct so that the yellow/red didn't burn, trying to encase them, and with glass compatability, so they are languishing in a box somewhere. I also discovered that I have virtually no talent for painting!
I have been looking at this screen printing method - looks pretty good, but cannot find it or anything similar in the UK. Take a look at the you tube video lower down on the page:
http://ezscreenprint.com/
Check out http://www.warmglass.com/screen_printing.htm
Modified to add, See also Rachel's post re Screen printing on Glass at
http://www.frit-happens.co.uk/forum/index.php?topic=42130.0
Screen printing is easy and the equipment I use and teach with I started off with in my one bed flat before I built my studio. Detail wise you can get very fine lines and the deposit of ink on the glass is really the thickest and most even you can get.
Yep I use the "print it yourself" decals. You do get some movement if you fire between layers of glass but they come out clean if you fire them on top.
I fire them at 700C.
If you want to decal between layers, fire your decal to the under layer first, then cap and fire again. You can take them to a higher temp once they are capped. If they go much above 700 uncapped then they fade.
Mmm sepia!
Oh, also it's a good idea to run a few blank prints through your printer first to warm it up a bit before you print your decal sheet. And remember to take the cover tissue off before putting in the printer!!!
PM if more questions :)
Oh you can always embellish with glassline pens if you want to (but don't put them directly under your decal, even if you pre-fire them first, as it won't stick properly as the glass surface will be bumpy)
Thank you for all the screen printing refs, I'll schedule some reading for today :)
...and thank you, Jane, for the tips. I did a butterfly which was underlaid with pre-fired Glassline paints and just the tip of one wing was missing, but I thought that was because I'd had to move the decal to get it into the right place and it may have got dirty so didn't stick properly. The decal that I capped (after tack firing to 704) actually turned out to have the best detail so far.
So many things to try, I'll be happy for quite a while :)
I have tried it printing on the bulk standard white glass with mixed success. One came out fine. One I must have used too high a temperature and was quite faded. One the decal moved and came out a mess. So a bit of practise is helpful! I thought Warm Glass suggested using fine clear powder between layers but as mentioned above, the decal may move and can distort. however, I didn't try the suggestion of fusing on the bottom layer first, so that may be worth trying at some point. Good luck :)
Yay! Glad it was helpful! Look forward to seeing what you make :)
I do a lot of decal work for coasters and pet memorials. I usually fire on regular stained glass because I can find it locally. For coe purposes I only fire pieces that came out of the same sheet. I don't have my schedule in front pf me but I fire to 1380 and hold 10 minutes. If you want to cap it you must fuse the decal and in an other firing add the cap.
I sell many coaster sets, these sets have local beaches and make nice presents.
I you would like to see the coasters click on the link below and go to the pictures on glass gallery.
https://www.google.com/search?q=proulxglassdesigns.com&ie=utf-8&oe=utf-8&aq=t&rls=org.mozilla:en-US:official&client=firefox-a&channel=sb
Bob
Hi,
I've been using the Photo fuse paper for a few years, and found a number of different uses, personalising gift tags, coasters, fridge magnets, and other bits and pieces.
I always fire between the glass, all in one fuse,
(http://farm8.staticflickr.com/7442/12741133334_4970ab8b31.jpg) (http://www.flickr.com/photos/89010559@N07/12741133334/)
IMAG0485[1] (http://www.flickr.com/photos/89010559@N07/12741133334/) by 1055Nina (http://www.flickr.com/people/89010559@N07/), on Flickr
I've had mixed results, but find it fun to play with.
(http://farm4.staticflickr.com/3709/12741135914_f5dc8ed830.jpg) (http://www.flickr.com/photos/89010559@N07/12741135914/)
IMAG0489[1] (http://www.flickr.com/photos/89010559@N07/12741135914/) by 1055Nina (http://www.flickr.com/people/89010559@N07/), on Flickr
Fridge magnets are an easy make and sell at craft fairs.......
If you zoom into the photo you can see that some of these have been fired at too high a temperature and the decal paper has started to move, so they will be consigned to the bin, but a few are okay and will end up with Magnets on the back........
I've just realised that I've been missing posts but I'm not sure how. Thank you for all your help, it's been really useful.
The pictures appear clearer (ie. sharper picture with better detail) when fusing between two sheets of glass rather than on top, and it's a lot more durable as well. I tried painting on top of one design to give a hand-tinted look, but the paint was all streaky and didn't look good at all. While cleaning it all off half the sepia came off as well, so I used a diamond pad to clear the whole lot off and fused a completely different photo on top of the resulting matt surface :)
Here are the two attempts that I've been most pleased with so far.
(https://v4s1.yimg.com/sj/2857/12903393084_8d6d9cc6db_n.jpg) (http://www.flickr.com/photos/73708665@N05/12903393084/)
Loughrigg Tarn (http://www.flickr.com/photos/73708665@N05/12903393084/) by Mead Moon (http://www.flickr.com/people/73708665@N05/), on Flickr
(https://v4s2.yimg.com/so/7448/12903063703_1ba0d1921e_n.jpg) (http://www.flickr.com/photos/73708665@N05/12903063703/)
Loughrigg Tarn reflections (http://www.flickr.com/photos/73708665@N05/12903063703/) by Mead Moon (http://www.flickr.com/people/73708665@N05/), on Flickr
Oh well done - they look really good ;)
Those look very, very good.
Thank you. They do need to be backlit though otherwise they are a bit dark and you can't see the detail, so any tips regarding framing, so that they could be hung in a window, or another method of backlighting would be welcome.
Those look good. I always read you could not cap them so I never tried, after seeing yours and Nina's I will have to try it.
Bob
Dee (chewsymums on you tube) gives some good hints on fusing decals