Post by: CelticGlass on November 26, 2007, 08:00:11 PM
Not sure if any ones spotted this before but its a short online movie of the Kiln being progammed for the variety of ramps for annealing glass.

http://www.paragonweb.com/VideoInfo.cfm?VID=2
Title: Re: Paragon Progamming Movie Online
Post by: glassworks on November 26, 2007, 08:13:06 PM
genius raymondo!!!!

;D ;D 8)
Title: Re: Paragon Progamming Movie Online
Post by: Lyn G on November 26, 2007, 08:25:33 PM
Ray,

Thanks so much for displaying that link - it has all become clear now!!  I have only been using my kiln for just over a week now and haven't programmed it at all.....apart from getting it to switch itself off about half an hour or so after I have finished for the evening.  No broken beads yet!!  :D

Anyway, after watching this I will definitely have a go!!

Thanks again.

Lyn
Title: Re: Paragon Progamming Movie Online
Post by: Kaz on December 04, 2007, 10:39:05 AM
Oh thanks for that - I have not started using my kiln yet and this is really helpful! Also the video on shelfwashing too!