Lampwork => Borosilicate => Topic started by: Tonyb on January 06, 2014, 01:01:31 PM

Title: Cutting boro tube
Post by: Tonyb on January 06, 2014, 01:01:31 PM
Hi,

I bought some boro tube and want to cut it into sections before putting it near a flame. I bought a cheap glass cuttter tool from B&Q with a small metal wheel but it's difficult to control and doesn't give a clean cut. Before spending more money on something that may not work, can someone recommend a better tool or method to cut the tube ?

Thanks

Tony
Title: Re: Cutting boro tube
Post by: jammie on January 06, 2014, 01:17:11 PM
I think when I was at my class Ian showe d me how to cut by scoring the tube with a scoring tool and then using spit on it then breaking it, but a boro person will come along soon to see if that's right.
Title: Re: Cutting boro tube
Post by: Ian Pearson on January 06, 2014, 02:13:45 PM
If you can get a tungsten carbide knife then that would be good. Just mark tube surface, a little spit as Jean says and bend and pull apart at same time. Dependent on length and diameter of course. Happy new Year everyone

Ian
Title: Re: Cutting boro tube
Post by: Redhotsal on January 06, 2014, 02:56:33 PM
Wonder if a pipe cutter would work?
Title: Re: Cutting boro tube
Post by: jammie on January 06, 2014, 04:11:14 PM
Happy new year Ian, hah I remembered my lesson right  ;D!
Title: Re: Cutting boro tube
Post by: Hamilton Taylor on January 06, 2014, 04:15:14 PM
Get a couple of these (http://www.diy.com/nav/decor/tiles/tiling-tools-accessories/cutting_tools/-specificproducttype-tile_scribes/B-and-Q-Tile-Scribe-9706814?skuId=10077547) - the blade is tungsten carbide, square section, so you have 4 cutting edges.
Make a short score on the glass, wet it, break by pulling apart with slight bending. Its a knack - try on rod first as its easier.

This site (http://www.ilpi.com/glassblowing/) is a pretty good resource for scientific glassblowing techniques, and if you look here (http://www.ilpi.com/glassblowing/tutorial_cutting.html) there is a cutting tutorial.

HTH,

Sean
Title: Re: Cutting boro tube
Post by: Ian Pearson on January 07, 2014, 08:36:44 AM
Come to Lybster on March 25th - 27th for my course and I will show you and guide you. Yes Jean those dates are OK so book now

Ian
Title: Re: Cutting boro tube
Post by: jammie on January 07, 2014, 11:20:24 AM
pmd you Ian!
Title: Re: Cutting boro tube
Post by: Tonyb on January 08, 2014, 12:23:04 PM
Thanks everyone for the suggestion and information. I will buy a couple of those tile scribes that Sean recommends next time i'm in B&Q. Will also try the pipe cutters as suggested by Sally and will let you know how I get on.

Tony