Lampwork => COE 104 => Topic started by: Purple Cobwebs on December 07, 2013, 06:47:25 PM

Title: Looking for tips on the new effetre Lilac Pastel and Lilac Dark Pastel
Post by: Purple Cobwebs on December 07, 2013, 06:47:25 PM
I ordered some of this last week and got to play with it tomorrow. All I've got out of it are boring pale grey beads! No difference between the lilac and the lilac dark.
I tried striking, zilch, and reducing, zilch!
How do I get lilac out of it?
I love lilac, but am not a fan of grey, so any help appreciated!!!!
Title: Re: Looking for tips on the new effetre Lilac Pastel and Lilac Dark Pastel
Post by: Kimster on December 11, 2013, 03:06:04 PM
Mine are just the same :(
Title: Re: Looking for tips on the new effetre Lilac Pastel and Lilac Dark Pastel
Post by: Enchanted Cobwebs on December 11, 2013, 04:12:25 PM
I have no advice but glad I didn't get tempted then with these!
I cant ever get anything nice out of anything claiming to be lilac or violet, usually get something with a grey oil slick finish that needs a dunk in etch all and even then its yukky!
Title: Re: Looking for tips on the new effetre Lilac Pastel and Lilac Dark Pastel
Post by: Jane C ♫ on December 11, 2013, 08:26:00 PM
Not the same colour, but I got some lovely effects out of the aubergine by basically boiling it on the rod for a bit! Try it?