Frit-Happens !

Lampwork => COE 104 => Topic started by: Kimster on December 06, 2013, 11:15:02 AM

Title: Can I make marbles from soft glass?
Post by: Kimster on December 06, 2013, 11:15:02 AM
I've just been asked if I can make a set of marbles to go in a wooden puzzle. I don't know if I can or not! :-\  Only one way to find out..
I can make a decent round bead & also have a beadroller. They don't need to be super dooper round as they're not for rolling, but it would be good practise for me  :)
Can anyone point me in the right direction for tut's etc? The only ones I can find seem to be boro..
Thanks all   :)
Title: Re: Can I make marbles from soft glass?
Post by: james M knox on December 06, 2013, 11:29:56 AM
Kimster,

I make marbles all the time from effetra (coe 104). I just take the borro instructions and do them in the softer glass.  ;D

One thing I would say is be very carefull to anneal the marble fully, I find it takes longer than i would normally do for beads, but then my marbles are about 15-25 mm diameter and my beads tend to be 15 or less mm.

If I get a chance I will take a few photos of my marbles (if I dont loose them  ;) ) and post them here.

James.
Title: Re: Can I make marbles from soft glass?
Post by: Steampunkglass on December 06, 2013, 11:45:31 AM
yes, I know that Drew Fritts did a book 'torchwork marbles' which was all soft glass. I think you can either use a boro punty which is the most popular way, or I have used a hot 3.2mm mandrel as a punty too, but I'm no expert, I find them harder to make as I'm just not used to soft glass much anymore  :-\ :-\ :-\ If you really want to get into them then maybe it'll be worth visiting Sean at Off Mandrel, he makes some lovely soft glass marbles
Title: Re: Can I make marbles from soft glass?
Post by: Nicknack on December 06, 2013, 11:57:58 AM
I just did a class last week at the Old Kennels, Dunkeswell, and on one day we made marbles.  We made soft glass ones in the morning, and a Boro one in the afternoon.  We used Boro punties for the soft glass ones, but it is possible with soft glass punties, as I made one at home, and didn't have any Boro.  As James says, just follow the Boro instructions, but use 104.  At least one of my 104 marbles exploded in the kiln on the course, but the one I made at home didn't.

Nick
Title: Re: Can I make marbles from soft glass?
Post by: Hamilton Taylor on December 06, 2013, 12:27:27 PM
Don't bother with glass punties, except for the very last one - use a 2.4 or 3.2mm mandrel instead.
Soft glass punties soften too easily at the connection point - you lose control.
Boro punties, there's a risk of leaving a bit of boro in a marble when detaching = kiln explosion.

"torchworked marbles" by Drew Fritts - can't recommend highly enough.

You can see some of my marbles here (http://www.flickr.com/photos/hamiltontaylor/sets/72157624489368119/) if you're interested - the vast majority are soft glass.

Have fun!

Sean  :)
Title: Re: Can I make marbles from soft glass?
Post by: Pat from Canvey on December 06, 2013, 12:42:18 PM
Beautiful marbles Sean. The lowest price I've found on Amazon UK for Drew Fritts book is £110 for a used copy. Are you by any chance offering a marbles course in 2014?
Title: Re: Can I make marbles from soft glass?
Post by: Hamilton Taylor on December 06, 2013, 01:10:52 PM
Wow. Drew is sold out too. He has some links you can try though, check his website (http://frittsartglass.com/marbles/books/volume1/TOC.html).

Meanwhile, I'm looking for a safe to keep my copy in!  :)

As to classes - I'm not hosting any, but am happy to teach if one of the teaching studios is interested.

Sean

Title: Re: Can I make marbles from soft glass?
Post by: Blue Box Studio on December 06, 2013, 01:13:21 PM
Would love to try marbles (seeing I have so few of my own) and didn't realise it was possible in soft glass.  Love those with the flowers Sean.
Title: Re: Can I make marbles from soft glass?
Post by: Kimster on December 06, 2013, 01:15:22 PM
Thanks all. Beautiful marbles Sean! Much more inspired now to give it a go - will hunt out the boro videos on youtube. Can't splash out on that book at this stage   :o :o
Title: Re: Can I make marbles from soft glass?
Post by: SilverGems89 on December 06, 2013, 03:20:37 PM
Pat I just took delivery of a brand new copy of torchworked marbles from artco. inc for $29.95 plus $24 postage (around £34 GBP)
here's a link for anyone interested in getting a copy
http://www.artcoinc.com/torchworkedmarbles.php

I don't know how many Malcolm has in stock but I assume he still has some as they are still listed on his site! Drop him an email and he'll sort you out  :) Mine arrived really quickly and managed to sneak past the customs radar  ;) Just about to sit and have a read now!
Title: Re: Can I make marbles from soft glass?
Post by: SilverGems89 on December 06, 2013, 03:23:51 PM
In response to Kimster, yes you can make marbles with 104, it is just more difficult to avoid thermal shocking than with boro  ;)
Check out the Marble and boro room on LE, lots of useful hints and tips and links to tutorials, but I have found a lot of videos on youtube to be very helpful!
Title: Re: Can I make marbles from soft glass?
Post by: Kimster on December 06, 2013, 05:37:15 PM
Thanks again - have dropped an email re the book  :)
Title: Re: Can I make marbles from soft glass?
Post by: Nicknack on December 06, 2013, 05:53:17 PM
Me too.

Nick
Title: Re: Can I make marbles from soft glass?
Post by: SilverGems89 on December 06, 2013, 05:55:06 PM
I believe Frantz have some too  ;)

ETA, Scrap that, looks like they are sold out  :( They had some when I ordered mine!
Title: Re: Can I make marbles from soft glass?
Post by: silkworm on December 06, 2013, 11:15:27 PM
And me! Except mines is for my husband, that and a marble mold will be his Christmas presents.
Title: Re: Can I make marbles from soft glass?
Post by: Miriam on December 07, 2013, 05:31:49 AM
I make soft glass marbles all the time. I use boro punties except for the last one, then I use a thin softglass punty. and as said, Drew's book is the book to read.

As for rounding, you could use a normal round mold, but the best tool ever to make round beads is the Infinite Rim Mold!!

You can see some of my marbles at my website: http://www.facet-design.com/wp/fotoalbums/album/72157628635484889/2012-2013-beads.html (http://www.facet-design.com/wp/fotoalbums/album/72157628635484889/2012-2013-beads.html)
Title: Re: Can I make marbles from soft glass?
Post by: Pat from Canvey on December 07, 2013, 07:07:19 AM
Thanks for posting the link Miriam. I especially like the one with the red flower near the bottom of the group.