Frit-Happens !

Lampwork => Borosilicate => Topic started by: SilverGems89 on November 20, 2013, 01:06:19 PM

Title: Tube for baubles
Post by: SilverGems89 on November 20, 2013, 01:06:19 PM
Hi everyone! I am feeling like being brave and having a go at blowing some baubles for Xmas, what tube would be the best size? And wall thickness?
Title: Re: Tube for baubles
Post by: Marcel on November 20, 2013, 07:18:09 PM
It depends a bit what your set up is  ;)
are you on tank or concentrator?
i use 24 mm wall thicknes 2,5 mm on concentrators i use
a bethlehem Alpha for that
and i use 30 mm wallthickness 2,8 on my bravo  8) and that is on tank
Title: Re: Tube for baubles
Post by: SilverGems89 on November 20, 2013, 07:37:41 PM
I've got an Alpha on a concentrator  ;D I'm torn between 18mm/2.5mm wall, 24mm/1.8mm wall or 24mm/2.5mm wall  :-\
Title: Re: Tube for baubles
Post by: garishglobes on November 20, 2013, 07:43:27 PM
I use 32mm with a 4mm wall thickness but have a big torch and a couple of large concentrators.

With a smaller set-up, I'd be tempted to go with either 24mm and 1.8mm-2.5mm wall or 18mm and 1.8mm wall. The size of tube will determine the size of the bauble to an extent.

I don't think it'll matter too much which you go for - I'm assuming the concentrator is 10l? If not, then I think I'd be tempted to go with the 1.8mm wall. The 1.8mm will melt a bit quicker so you'll lose on the control front but set against that, you'll gain because it'll soften quicker if you have less heat, if that makes sense.

Title: Re: Tube for baubles
Post by: Lotti on November 20, 2013, 07:47:02 PM
Quote from: garishglobes on November 20, 2013, 07:43:27 PM
I use 32mm with a 4mm wall thickness but have a big torch and a couple of large concentrators.

With a smaller set-up, I'd be tempted to go with either 24mm and 1.8mm-2.5mm wall or 18mm and 1.8mm wall. The size of tube will determine the size of the bauble to an extent.

I don't think it'll matter too much which you go for - I'm assuming the concentrator is 10l? If not, then I think I'd be tempted to go with the 1.8mm wall. The 1.8mm will melt a bit quicker so you'll lose on the control front but set against that, you'll gain because it'll soften quicker if you have less heat, if that makes sense.



I have the 18 with a 1.8 wall.  ;) :)
Title: Re: Tube for baubles
Post by: SilverGems89 on November 20, 2013, 08:15:16 PM
Thanks everyone, I think I will go with the 1.8mm wall thickness, will ponder the diameter a bit more  :)