Hi All
I just wanted to warn anyone who bought CIM Trade Winds that they might want to go slow with it until checking compatibility.
I made some simple nuggets using three transparent glasses in a single bead: Effetre Grass Green, Effetre Light Turquoise and CIM Trade Winds.... and compatibility cracks have now formed in 3 out of the 7.
Very much doubt it's the Effetre, as both are tried and tested, and I haven't bought a new batch of either Effetre colour recently. ::)
Just letting people know to tread cautiously with this glass.