Frit-Happens !

Lampwork => Borosilicate => Topic started by: Lotti on October 18, 2013, 01:06:14 PM

Title: Torch
Post by: Lotti on October 18, 2013, 01:06:14 PM
Right, so as a new boro convert I am thinking torches! (I have a 10l oxy and also actually still have my old 4L one too).  I was thinking Lynx as I quite like the fact that A) I can get it in the UK and B) you can adjust the flame.  But....  Tufnells don't seem to have them at the mo and anyway I was wondering about the Bethlehem torches.  The Alpha is more affordable, but will I get fed up with it before too long and want to upgrade and is it any good with boro (I know it says it is), then there is the Bravo, but it is lots and lots of pennies, but would it be more sensible (!!!!!!!!!!!!!!!!!!!!!) or should I import something from the US (also !!!!!!!!!!!!!!!!!!!!!!!!).  I have a minor which I suppose I could just play with to start with, so not in a great rush? All advice greatly welcomed :)
Title: Re: Torch
Post by: Kalorlo on October 18, 2013, 02:42:40 PM
Depends how big you want to work? I am finding my Minor fine for the time being. (I think I might like a Lynx eventually, but it'd be nice to have a go on one somehow beforehand!)
Title: Re: Torch
Post by: Steampunkglass on October 18, 2013, 03:31:53 PM
I was on a minor for ages and it was fine with two oxys on boro, you should have no problems with a 10l oxycon, it's amazing how much power you can get out of a minor so I wouldn't worry about rushing to upgrade yet. It also depends on what type of thing you want to make, as some torches seem to have wider flames for blown work  ???
Title: Re: Torch
Post by: Lotti on October 18, 2013, 05:03:31 PM
Thanks folks.  I will be wanting to move onto blown (you should have seen my attempts yesterday, or maybe not, but it's all learning!).  Have just been eyeing up a couple of other GTT torches from a chap on Ebay (a shop that is), um..... ;)  But I will be good and not rush into anything, honest ;) :)
Title: Re: Torch
Post by: ARBeads on October 18, 2013, 05:15:34 PM
I'm using the MidRange, finding no problems blowing - nice bushy flame. Not really used much silver colour yet so not sure if it will be 'man enough' to get the super boro colours. I'm daisy chaining 2 5lt oxycons without to many problems. Going to add more in the NewYear  ::)

Title: Re: Torch
Post by: fionaess on October 18, 2013, 07:13:14 PM
I have a GTT Scorpion with 2 oxycons - just wish I had your 10 litre just to see what my torch can really do  ;D
Title: Re: Torch
Post by: Barnacle Bay on October 18, 2013, 07:57:16 PM
This is a very interesting topic... I have only been playing with Boro for just  under 2 months  using my minor & 5 ltr oxy.  I nearly bought another 5ltr oxy as what I had read/told that working with Boro on such a simple set up was going to be a nightmare although fine for 5 to 6mm rods and anything and above that then I would need a bigger girls torch and another oxy :-\   Anyway, I have tried it out and have to say (although you have the 10 ltr oxy - which must be bliss)  I have had no problems at all.  I have been working with rods from 6mm up to 15 mm and can say they do melt quite easily on my 5 ltr oxy and my Minor. 

Corina Tettinger has most (if not all torches) which she has reviewed, inc Nortel Minor Burner
Lynx
Bobcat
Piranha
Wale Firebird
Carlisle Mini CC
Carlisle Bunsen Burner
Hothead

Reviews:  http://www.corinabeads.com/pages/torchreview.php

I read on the Nortel Minor site that the Minor can work up to 3 inch beads, I think that is another factor why I bought it:   http://www.nortelglass.com/torches-minor.shtml

Louxx
Title: Re: Torch
Post by: garishglobes on October 19, 2013, 08:26:48 AM
When it comes to using boro and making sculptural work/blowing, it seems to me that you require several different things from the torch and that it is hard to find a torch that combines all of them. As a result, the torch may well be a compromise that works best for the things you do most.

With boro, you work hot. But for blowing, you want a soft, wide flame. Probably most of the time, you blow clear glass so flame atmosphere isn't so much of an issue. However, I think many torches that have this soft, wide flame also have a more reducing atmosphere. For sculpture, a slightly less soft, wide, hot flame is nice for getting the thing going but you would also be looking at wanting a pinpoint flame and to be able to adjust between the types of flame quickly and with ease. Again, if you are mainly sculpting in clear, flame atmosphere wouldn't be an issue. If you are planning on using the colour-changing, metal-rich colours, you want to be able to get as much of a neutral flame as possible to get the most out of the colour as you can. There are ways to help with this, like encasing the colour to protect against the atmosphere, but a neutral flame is still nice if you can get it.

Personally, I think the Midrange is probably a very nice torch for blowing but I struggle with flipping it between the wide flame and a pinpoint one for sculpture and for doing things like straightening points. I'm just too impatient and I like to be able to go from wide to narrow quickly! From experience, I also think that it has quite a reducing flame (the one I had was muddying Bullseye pinks, with a new 8l oxycon!) but that could well just be the torch I was using  ;)

Some of the GTT torches are designed to get the best out of oxycons and they do in general seem to run a much cleaner, more neutral atmosphere. But the range of flame isn't always ideal and they don't do soft, wide and bushy (at least, not until you are paying quite a lot!!) so aren't the perfect blowing torch. Having said that, I use one because of the clean flame and the ease of switching between narrow and wide flame and I blow by working away from the torch head.

I don't know much about the Bethlehems or the Carlisles, not enough to comment. But even the Herbert Arnold, which would be my idea of the ultimate perfect compromise, has quite a reducing atmosphere - and it would only run on an oxygen tank.



Title: Re: Torch
Post by: Hamilton Taylor on October 19, 2013, 08:41:41 AM
With many of the boro reactive colours, to really get them to pop, you need an oxidising flame. It's very difficult to get good colour using oxycons, even working small - but it can be done. I agree with Emma - a soft, wide, pointy, narrow flame is ideal...  ;D

Sean
Title: Re: Torch
Post by: Lotti on October 19, 2013, 09:35:58 AM
I think it will be a GTT for me in some form or other.  I think (early days) that I will be looking for one that can go easily between a big soft flame and a pointy one.  Been eyeing up a Scorpion which apparently likes a 10L oxy (as I say I still have my old 4L so if need be could always link that up too!!!).  Will start on my old minor for a bit (need to save some pennies first) and look at the reviews, but this has been very helpful to me and hopefully to others.  Maybe a sticky on torches Emma ;) :)
Title: Re: Torch
Post by: ajda on October 19, 2013, 02:31:37 PM
Oxygen is the key to the power (and flexibility) you need if you want to get the best out of boro. We have 2 x 10L oxycons from Unlimited Oxygen in the US. Jack Ridgway of Unlimited Oxygen is a law unto himself and very frustrating to deal with - it took 6 months to get them here, but in the end was worth the wait. We have them linked together feeding 2 torches - a Carlisle Mini CC and a Bethlehem Bravo (both also bought direct from the US). With plenty of oxygen, both are good for boro - though the CC is obviously more limited. We often use both torches at the same time, but for maximum power I like the Bravo with both oxycons to itself.

I love both those torches, but if I was 30 years younger and not so lazy I think I could get into torch design - we could do with some good UK rivals to these American torch makers.

Alan

Title: Re: Torch
Post by: garishglobes on October 19, 2013, 04:03:22 PM
Oh my goodness, don't get me started on Unlimited Oxygen.... beyond frustrating to deal with and between them and the shipper, oxycon absolutely not guaranteed to arrive in one piece  >:(  Sounds like you were lucky!
Title: Re: Torch
Post by: ARBeads on October 19, 2013, 04:15:58 PM
I've got the 10 ltr from Unlimited Oxygen in bits, most of the vent/changeover ports are filled with silicon grease  - slowly working my way through cleaning all the grease from the valves and switches. There is no way this would ever have worked even if the compressor base had been in one piece. Having looked at this one I wouldn't touch them with a barge pole!



Title: Re: Torch
Post by: garishglobes on October 19, 2013, 05:33:08 PM
Good grief!! Sounds as if I gave you quite a project.
Title: Re: Torch
Post by: ajda on October 19, 2013, 08:12:39 PM
Wow! I thought I'd had a hard time with Jack of Unlimited Oxygen, but it sounds as if I got off lightly... As regards shipping, I had excellent service from patrick.amoroso@dhx.com and wouldn't hesitate to use again.
Title: Re: Torch
Post by: tinker on October 20, 2013, 10:22:44 AM
Thanks for this really informative post, I've been wanting to play with boro too :)

Does anyone have any experience or advice with regards to working it on a cricket? I plan to get another oxy in the new year but wasn't really sure whether I need to hold out for a bigger torch too or whether I'd be content for the time being on the cricket.
Title: Re: Torch
Post by: jammie on October 20, 2013, 05:56:41 PM
Tan did a post (not sure where though) of working boro on one oxy, I can manage 9mm rods on a bobcat and one oxy so think you would be ok ! but that is only clear, haven't tried colour yet. Just waiting for xmas to order some clear from Sean!  :)
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible? I was going for another oxycon but didn't have enough money when it came to it so will just ave to ait and make do with what I have for now.
Title: Re: Torch
Post by: Steampunkglass on October 20, 2013, 07:33:01 PM
Quote from: jammie on October 20, 2013, 05:56:41 PM
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible?
I knew that the oldest one of my two oxys was on the way out when I got more of a reducing atmosphere as the day's work went on, even though the dial was still saying it was producing enough pressure after a few hours anything with turbo cobalt was going ashy grey. If it's old perhaps it's not producing as pure an oxygen output anymore?  ??? ??? ???
Title: Re: Torch
Post by: jammie on October 20, 2013, 07:35:16 PM
It was 2nd hand but fine when I bought it, its the white and blues and pinks and anything that can go metallic. I thought another oxy would sort it and i could do more boro too, sadly my bankie was empty! :)
Title: Re: Torch
Post by: liquidglass on October 21, 2013, 03:08:02 PM
Quote from: jammie on October 20, 2013, 05:56:41 PM
Tan did a post (not sure where though) of working boro on one oxy, I can manage 9mm rods on a bobcat and one oxy so think you would be ok ! but that is only clear, haven't tried colour yet. Just waiting for xmas to order some clear from Sean!  :)
My bobcat is still giving me a reducing flame and am struggling to get the oxy to give out enough, some seem to have more output than others is that possible? I was going for another oxycon but didn't have enough money when it came to it so will just ave to ait and make do with what I have for now.

Just a quick note:

Tan's post for working on one oxycon is here - http://www.meltinglass.co.uk/article.php?xArt=8