Frit-Happens !

Lampwork => COE 104 => Topic started by: noora on September 02, 2013, 02:14:11 PM

Title: Best transparent red?
Post by: noora on September 02, 2013, 02:14:11 PM
What's the best behaved transparent red (not pink red like rubino, but plain red)? I can't get the striking effetre reds to behave, either they don't strike properly or they turn murky :P Sometimes both at once - one bit won't strike and another bit has already turned murky ??? So are there any easier transparent reds out there?

I'm trying to pull complex stringer with transparent red in it, which makes it even harder to get it "just right" in the end :-\
Title: Re: Best transparent red?
Post by: dinah46 on September 02, 2013, 02:16:32 PM
I love Cim Sangre, it does need striking but I find it strikes quite easily
Title: Re: Best transparent red?
Post by: Trudi on September 02, 2013, 04:24:38 PM
Quote from: dinah46 on September 02, 2013, 02:16:32 PM
I love Cim Sangre, it does need striking but I find it strikes quite easily

Me too  - but in larger beads it does tend to go opaque!

- one of the new CiM reds is also supposed to be nice, but I've not got my hands on them yet!

Maraschino - is lovely but is opaque
Title: Re: Best transparent red?
Post by: Madam Steph on September 02, 2013, 07:31:02 PM
Maraschino is my best ever red


L x
Title: Re: Best transparent red?
Post by: MangoBeads on September 02, 2013, 08:29:06 PM
I love Lausha transparent Red :)
Title: Re: Best transparent red?
Post by: Calico Cat on September 02, 2013, 09:08:16 PM
Quote from: MangoBeads on September 02, 2013, 08:29:06 PM
I love Lausha transparent Red :)

Thanks for the reminder - just gone and ordered some  ;D
Title: Re: Best transparent red?
Post by: MangoBeads on September 02, 2013, 10:19:20 PM
:)
Title: Re: Best transparent red?
Post by: ARBeads on September 02, 2013, 11:48:00 PM
My favourite transparent was/is a Reichenbach 104 just labelled transparent red - I used it for spacers and mourn the day I got down to my last 1/2 rod, it's fondled lovingly and promised friends but so far I've been unable to find anything quiet like it  ::)
Title: Re: Best transparent red?
Post by: noora on September 03, 2013, 07:45:27 AM
Thank you for the suggestions :) According to my list I actually have some CIM Sangre. Now I just have to locate it in my rod shelf... I buy more glass than I have time to try out ::)

Where can I buy Lausha?
Title: Re: Best transparent red?
Post by: Princess Peggy (Priscilla McGirr) on September 03, 2013, 08:10:12 AM
In a stringer you are always going to have trouble getting a transparent red to show up, specially the striking ones.  I would try Effetre Light Red 591428......if you are going to thin it down it has a slightly translucent quality.
Title: Re: Best transparent red?
Post by: helbels on September 03, 2013, 09:04:08 AM
You can buy lauscha at www.lauscha.co.uk

- Although it looks like the website is down at the moment (or at least it is for me!)
Title: Re: Best transparent red?
Post by: Kalorlo on September 03, 2013, 09:16:30 AM
It's there for me at the moment - if anyone else is having a problem, can you let me know?
Title: Re: Best transparent red?
Post by: Jellybean on September 03, 2013, 09:21:36 AM
Not there for me either...
Title: Re: Best transparent red?
Post by: Kalorlo on September 03, 2013, 09:41:44 AM
If you go to http://lauscha.heatherkellyglass.co.uk/ instead, is it there? Or to http://lauscha.heatherkellyglass.co.uk/catalog/rods/transparent ?

That is weird.
Title: Re: Best transparent red?
Post by: ruth on September 03, 2013, 09:46:28 AM
 not there for me either.
Title: Re: Best transparent red?
Post by: helbels on September 03, 2013, 09:47:38 AM
The second link works for me Heather, but the first one is giving a "Page Not Found" error.
Title: Re: Best transparent red?
Post by: Essex Girl on September 03, 2013, 09:54:07 AM
Quote from: helbels on September 03, 2013, 09:47:38 AM
The second link works for me Heather, but the first one is giving a "Page Not Found" error.
Same for me.
Title: Re: Best transparent red?
Post by: Kalorlo on September 03, 2013, 09:59:45 AM
That is really bizarre, will have to see if I can fiddle with anything tonight.
Title: Re: Best transparent red?
Post by: flame n fuse on September 03, 2013, 11:19:10 AM
both links are working for me!
Title: Re: Best transparent red?
Post by: Essex Girl on September 03, 2013, 11:42:54 AM
Working for me now :)