Do any of you know the answers to a couple of questions?
1. How long from closing the kiln door and running the batch anneal for SC2 detailed above can I open the door and take my beads out?
2.Does anyone know how much it costs money-wise to run a batch annealing cycle in the SC2?
Ta loves,
KJ.
the beads can come out when they have cooled enough to carry - anything under 50 degrees C is about as long as griet has ever been able to last!!
;D ;D
the annealing cycle costs pennies - the kilns are efficient and very well insulated..
;)
Lovely, thanks Q. Griet is a girl after my own heart, I have to physically stop myself opening the door too soon!!!